Next Article in Journal
Al–Fe–Si–La Alloys for Current Collectors of Positive Electrodes in Lithium Ion Batteries
Next Article in Special Issue
Metals in Hydrogen Technology
Previous Article in Journal
Leaching Chalcopyrite with High MnO2 and Chloride Concentrations
Previous Article in Special Issue
A Heterothermic Kinetic Model of Hydrogen Absorption in Metals with Subsurface Transport
 
 
Font Type:
Arial Georgia Verdana
Font Size:
Aa Aa Aa
Line Spacing:
Column Width:
Background:
Correction

Correction: Ono, S., et al. A Heterothermic Kinetic Model of Hydrogen Absorption in Metals with Subsurface Transport. Metals, 2019, 9(10), 1131

1
Department of Chemical Engineering, Kyoto University, Nishikyo, Kyoto 615-8510, Japan
2
Department of Chemical Engineering, University of Manchester, Oxford Rd, Manchester M13 9PL, UK
3
Graduate School of Advanced Integrated Studies in Human Survivability, Kyoto University, Sakyo, Kyoto 606-8306, Japan
*
Author to whom correspondence should be addressed.
Metals 2020, 10(1), 108; https://doi.org/10.3390/met10010108
Submission received: 7 January 2020 / Accepted: 9 January 2020 / Published: 9 January 2020
(This article belongs to the Special Issue Metals in Hydrogen Technology)
The authors wish to make the following corrections to this paper [1]:
1. In the first line of Page 11, we need to modify the values
  • ksb0 = 1.4 × 1013 s−1 into ksb0 = 5.8 × 1012 s−1
  • kbs0 = 6.2 × 1012 s1 into kbs0 = 7.6 × 1011 s1.
The same thing applies in the figure captions of Figures 12 and 13.
(Reason) By accident, we presented the wrong set of numbers. Therefore, we need to correct them for the readers, otherwise no one would be able to reproduce our calculation results with the correct parameter values. Nevertheless, we confirm that all the calculations we performed were carried out with the correct values, and therefore none of the results, figures, or conclusions in the paper were affected.
2. We need to specify that the results presented in Figure 15 are for a temperature of 25 °C.
(Reason) We omitted presenting at which temperature the calculations in Figure 15 were carried out. This information is indispensable, because the results presented in Figure 15 significantly depend on the temperature, and thus Figure 15 would not make sense without specifying the temperature.
These points listed are small, but important and have a significant influence, and therefore we have revised them. The authors would like to apologize for any inconvenience caused to the readers by these changes.
We will update the article and the original version will remain available on the article webpage.

Reference

  1. Ono, S.; Uchikoshi, T.; Hayashi, Y.; Kitagawa, Y.; Yeh, G.; Yamaguchi, E.; Tanabe, K. A heterothermic kinetic model of hydrogen absorption in metals with subsurface transport. Metals 2019, 9, 1131. [Google Scholar] [CrossRef] [Green Version]

Share and Cite

MDPI and ACS Style

Ono, S.; Uchikoshi, T.; Hayashi, Y.; Kitagawa, Y.; Yeh, G.; Yamaguchi, E.; Tanabe, K. Correction: Ono, S., et al. A Heterothermic Kinetic Model of Hydrogen Absorption in Metals with Subsurface Transport. Metals, 2019, 9(10), 1131. Metals 2020, 10, 108. https://doi.org/10.3390/met10010108

AMA Style

Ono S, Uchikoshi T, Hayashi Y, Kitagawa Y, Yeh G, Yamaguchi E, Tanabe K. Correction: Ono, S., et al. A Heterothermic Kinetic Model of Hydrogen Absorption in Metals with Subsurface Transport. Metals, 2019, 9(10), 1131. Metals. 2020; 10(1):108. https://doi.org/10.3390/met10010108

Chicago/Turabian Style

Ono, Shunsuke, Takeru Uchikoshi, Yusuke Hayashi, Yuta Kitagawa, George Yeh, Eiichi Yamaguchi, and Katsuaki Tanabe. 2020. "Correction: Ono, S., et al. A Heterothermic Kinetic Model of Hydrogen Absorption in Metals with Subsurface Transport. Metals, 2019, 9(10), 1131" Metals 10, no. 1: 108. https://doi.org/10.3390/met10010108

Note that from the first issue of 2016, this journal uses article numbers instead of page numbers. See further details here.

Article Metrics

Back to TopTop