Next Article in Journal
Engineering SERS Properties of Silicon Nanotrees at the Nanoscale
Next Article in Special Issue
New ICT-Based Ratiometric Two-Photon near Infrared Probe for Imaging Tyrosinase in Living Cells, Tissues, and Whole Organisms
Previous Article in Journal
Pithecellobium dulce Leaf-Derived Carbon Dots for 4-Nitrophenol and Cr(VI) Detection
Previous Article in Special Issue
Microstructure and Photoluminescence of ZrTiO4:Eu3+ Phosphors: Host-Sensitized Energy Transfer and Optical Thermometry
 
 
Font Type:
Arial Georgia Verdana
Font Size:
Aa Aa Aa
Line Spacing:
Column Width:
Background:
Article

Preparation and Photoluminescent Properties of Tb3+-Doped Lu2W3O12 and Lu2Mo3O12 Green Phosphors

1
Fujian Key Laboratory of Functional Materials and Applications, School of Materials Science and Engineering, Xiamen University of Technology, Xiamen 361024, China
2
Department of Fundamental Courses, Xiamen Donghai Institute, Xiamen 361112, China
*
Author to whom correspondence should be addressed.
Chemosensors 2022, 10(12), 533; https://doi.org/10.3390/chemosensors10120533
Submission received: 21 October 2022 / Revised: 12 December 2022 / Accepted: 12 December 2022 / Published: 14 December 2022
(This article belongs to the Special Issue Advances in Fluorescence Sensing)

Abstract

:
Tungstate and molybdate phosphors have received great attention for their excellent photoluminescent properties and thermal stabilities. In the article, Tb3+-activated tungstate and molybdate green phosphors were prepared by a solid-state reaction method at different caline temperatures and were compared and studied. The crystal structures and the morphologies of samples were characterized by X-ray diffraction (XRD) patterns and field emission scanning electron microscopy (FE-SEM) images. The energy-dispersive spectra (EDS) proved the compositions of the prepared samples. The photoluminescence (PL) spectra showed that the PL excitation spectra of Tb3+-doped Lu2W3O12 and Lu2Mo3O12 green phosphors consisted of a broad and strong charge transfer band (CTB) and 4f–5d transitions of Tb3+ in the ultraviolet (UV) wavelength range and some narrowed excitation peaks from the 4f–4f transition of Tb3+ in the near ultraviolet (NUV) wavelength region. The PL emission spectra of the phosphors exhibited the characteristic green emissions owing to the 5D47F5 transition of Tb3+ located at about 547 nm. The values of energy gap Eg were calculated based on the diffuse reflection spectra (DRS). The measuring temperature-dependent PL spectra illustrated the thermal stabilities of phosphors. The Tb3+-doped Lu2Mo3O12 phosphor presented normal thermal quenching phenomena and the values of the thermal activation energy Ea were calculated based on the measuring temperature dependent PL emission spectra. The Tb3+-doped Lu2W3O12 phosphor exhibited abnormal thermal enhancing CTB excitation intensity at about 170 °C. Furthermore, the PL decay curves suggested that the lifetime corresponding to the 5D4 level of Tb3+ in the Lu2W3O12 host lattice was longer than that in the Lu2Mo3O12 host lattice. Compared the Tb3+-doped Lu2Mo3O12 phosphor, the Tb3+-doped Lu2W3O12 phosphor has shown potential as an application in temperature sensors.

1. Introduction

In recent years, “double carbon” has once again become a hot topic, and many have made contributions to energy conservation and carbon reduction, saving electric energy more effectively and helping to achieve the goal of “double carbon”. As far as illumination is concerned, the key lies in the correct selection of high-efficiency phosphors that can emit good visible light. This requires the luminous efficiency and working stability of fluorescent phosphors. Phosphors have strong practical and scientific interest for scientists. Much of the literature concerning rare earth phosphors has reported on its wide applications [1,2,3,4]. Phosphors are classified by matrixes such as oxides, nitrides, phosphates, fluorides, borates, sulfates, aluminates, silicates, sulfides, tungstates, vanadates, molybdates, etc. Host materials with the values of energy band gaps Eg between 3 eV and 5 eV are considered to be the best host matrix for phosphors [5]. Among these phosphors, tungstate phosphors and the molybdate phosphors are considered to be promising phosphors, owing to their high physical and chemical stability as well as thermal stabilities [6,7]. In addition, the WO42−, WO66−, MoO42−, and MoO66− groups can efficiently absorb ultraviolet (UV) light through the excitation of the O2−−W6+ and O2−−Mo6+ charge transfer absorption [8,9,10,11]. The excitation energy can be transferred to luminescent ions, such as Eu3+ and Sm3+, and then emit red light. There are some reports on rare earth molybdate phosphors and tungstate phosphors [12,13,14].
Few reports on Tb3+-doped molybdate phosphors or tungstate phosphors were reported [15,16]. The Tb3+-doped materials are usually used as green phosphors because of their bright 5D47F5 emissions, which peak at about 544 nm in the green spectral region. To the best of our knowledge, the investigations on the Tb3+-doped Lu2W3O12 and Lu2Mo3O12 phosphors have been rarely reported. For phosphors, thermal quenching is a normal phenomenon for nonradiative transitions at higher temperatures, which is also a drawback for practical applications such as display, lighting, and photovoltaics [17]. Recently, thermally stable phosphors that conquered or were weak were reported as drawbacks [18,19]. Further, thermal enhancement up-conversion emissions in Yb2W3O12 and Sc2Mo3O12 materials were reported and the enhancement was attributed to the negative thermal expansion (NTE) [20,21]. When the up-conversion materials are integrated into biological sensors or optoelectronic devices, the thermally enhanced up-conversion luminescence can provide enhanced detection sensitivities and improved energy conversion efficiencies. Enhanced Eu3+ emissions were also reported in Lu2(MoO4)3 phosphors [22,23]. Above 450 K, the Lu2(MoO4)3 shows a very intense NTE phenomenon [24]. What about the Tb3+ emission in Lu2W3O12 and Lu2Mo3O12 host matrices?
In this work, the Tb3+-doped and undoped Lu2W3O12 and Lu2Mo3O12 green phosphors were prepared through a solid-state reaction method. The crystalline structures, the morphologies, the compositions, the diffuse reflectance spectra, the room temperature and high temperature photoluminescence spectra, the thermal stabilities, and the luminescent decay curves of Tb3+-doped Lu2W3O12 and Lu2Mo3O12 green phosphors were compared and studied.

2. Experimental Section

2.1. Materials

Lu2O3 (99.99%, Aladdin), Tb4O7 (99.99%, Aladdin), WO3 (99.99%, Aladdin), and MoO3 (99.9%, Aladdin) were used as raw materials without further purification to prepare the Tb3+-doped and undoped Lu2W3O12 and Lu2Mo3O12 materials.

2.2. Preparation and Characterization

The Tb3+-doped and undoped Lu2W3O12 and Lu2Mo3O12 materials were prepared through a solid-state reaction method as reported [22,23]. In a typical procedure, for the preparation of 10 mmol of 5 mol% Tb3+-doped Lu2W3O12, 9.5 mmol of Lu2O3, 0.25 mmol of Tb4O7, and 30 mmol of WO3 were weighed and ground thoroughly, placed into a corundum crucible, and calcined at 1000 °C for 4 h in a muffle furnace with some carbon powder in the muffle furnace. When the muffle furnace cooled down to room temperature, the obtained white powder was collected and the phosphor was obtained. For comparison, the 5 mol% Tb3+-doped Lu2Mo3O12 and undoped Lu2W3O12 and Lu2Mo3O12 samples were prepared with the similar procedure except for the raw materials. Calcining temperatures of 800, 900, 1000, 1100, 1200, and 1300 °C were applied to prepare the materials. Under 254 nm or 365 nm UV light, the Tb3+-doped materials emit a bright green light seen by the naked eye, suggesting green phosphors were prepared.
To determine the crystal structure, the X-ray diffraction (XRD) patterns of the prepared phosphors were characterized with CuKα (λ = 1.5406 Å) radiation at 40 kV and 40 mA using a Rigaku Smart lab X-ray diffractometer. The 2θ ranges of the data were all set from 10° to 70° with a step size of 0.02°. A Zeiss field emission scanning electron microscope (FE-SEM) was used to study the morphologies and the particle size. The compositions of the materials were characterized by energy-dispersive spectra (EDS) with the attachment EDS equipment in the FE-SEM. The diffuse reflection spectra (DRS) were obtained on a visible-near infrared (Vis-NIR) spectrophotometer (UV-2700) with BaSO4 as the standard reference. A Scientific Lumina fluorescence spectrophotometer with a power of 150 W Xe lamp as an excitation source was used to record the photoluminescence (PL) excitation and emission spectra at room temperature. The high temperature dependent PL spectra of obtained phosphors were recorded by the same fluorescence spectrophotometer with a heating equipment TAP-02 (Tian Jin Oriente KOJI Instrument Co., Ltd., Tianjin, China) high-temperature fluorescence attachment. The luminescent decay curves were recorded by a Horiba Scientific FluroMax-4 spectrophotometer with a pulsed 150 W xenon lamp as an excitation source.

3. Results

3.1. Characterization of XRD and Crystal Structure

Figure 1 shows XRD patterns of Tb3+-doped Lu2W3O12 phosphors prepared at 800, 900, 1000, 1100, 1200, 1300 °C, and reference data. The XRD patterns can be indexed to the Yb2Mo3O12 with JCPDS card No. 33-1451. Because Lu3+ is isostructural to the Yb3+ and the W6+ has similar electronic structure to that of the Mo6+, it can be inferred that the Lu2W3O12 phosphor was prepared. When the preparation temperature was 800 °C, the XRD pattern of the obtained material could be indexed to the reference data of Yb2Mo3O12 well. When the preparation temperature increased with 100 °C intervals up to 1300 °C, all the XRD patterns could be indexed to the reference data. The full width at half maximum (FWHM) of the diffraction peak became narrower and the diffraction intensity became stronger with the increase of preparation temperature. The XRD measurement results suggested that the Tb3+-doped Lu2W3O12 phosphors can be prepared from 800 °C to 1300 °C.
The preparation of temperature-dependent XRD patterns of Tb3+-doped Lu2Mo3O12 phosphors and the reference data are shown in Figure 2. Based on the analysis of [23] and the measurement results, the XRD patterns of Tb3+-doped Lu2Mo3O12 phosphors prepared at different preparation temperatures can all be well indexed to the reference data of Yb2Mo3O12 with JCPDS card No. 33-1451. Similar to those of the Tb3+-doped Lu2W3O12 phosphors, with the increase of preparation temperature, the full width at half maximum of the XRD diffraction peak became narrower and the diffraction intensity gradually increased. The results show that the Tb3+-doped Lu2Mo3O12 phosphors were obtained when the preparation temperature varied from 800 °C to 1300 °C.
Figure 3 shows the XRD patterns of 5 mol% Tb3+-doped and undoped Lu2W3O12 and Lu2Mo3O12 powders prepared at 1000 °C and the reference data. Referring to the preparation of the temperature-dependent XRD patterns of Tb3+-doped Lu2W3O12 and Lu2Mo3O12 phosphors, the XRD patterns of the 5 mol% Tb3+-doped and undoped Lu2W3O12 and Lu2Mo3O12 samples can be well indexed to Yb2Mo3O12 with JCPDS card No. 33-1451. Comparing the Tb3+-doped and undoped XRD patterns of the Lu2W3O12 and Lu2Mo3O12 powders, the Tb3+ doping did not cause apparent variations on the patterns, with the exception of the diffraction intensities.
Figure 4a,b display schematic crystal structure diagrams of Lu2W3O12 and Lu2Mo3O12, respectively. As is illustrated, Lu3+ is bonded to six O2− to form LuO6 octahedra and W6+ or Mo6+ is bonded to four O2− to form WO42− or MoO42− tetrahedra. The Lu2W3O12 or Lu2Mo3O12 crystal is composed of corner-sharing LuO66− octahedra and WO42− or MoO42− tetrahedra. One LuO6 octahedra shares corners with six WO4 tetrahedra. With the temperature increasing, the Lu-O-W and Lu-O-Mo will rotate, resulting in the shrinkage of the Lu2W3O12 and Lu2Mo3O12 crystal lattice, which present the NTE phenomena. After doping 5 mol% Tb3+, the Tb3+ ions replace the Lu3+ ions in the Lu2W3O12 and Lu2Mo3O12 crystals for the similarity of Tb3+ to Lu3+. The contraction of the crystal lattice will affect the emissions of Tb3+ at high temperatures.

3.2. Composition and Morphology Characterization

Figure 5 presents the FE-SEM images and EDS spectra of an undoped Lu2Mo3O12 sample (a,b), a 5 mol% Tb3+-doped Lu2Mo3O12 phosphor (c,d), undoped Lu2W3O12 material (e,f), and a 5 mol% Tb3+-doped Lu2W3O12 phosphor (g,h) prepared at 1000 °C, respectively. For convenient comparison, the scales bars were all 2 μm in the FE-SEM images, and all the FE-SEM images were captured under the same magnifications. The undoped Lu2Mo3O12 micron particles in Figure 5a were well dispersed with good homogeneity, non-agglomeration, uniformity in size distribution, and with a sphere-like morphology. Through a Nano Measurer software dealing, the average size of the particles was about 2.14 μm. The corresponding EDS spectrum in Figure 5b indicates that the material contains Lu, Mo, and O. After some Tb3+ was introduced into Lu2Mo3O12 lattice, the morphology of the micro-particles (Figure 5c) did not change much and the average size of the particles was about 2.17 μm. Tb3+ was detected in the corresponding EDS pattern (Figure 5d). The Lu2W3O12 was composed of some undefined and unsmoothed particles and some irregular agglomeration nanoparticles appeared on the surface of the particles (Figure 5e). Compared with Lu2Mo3O12 material, the Lu2W3O12 sample possessed smaller particles and the average size of the particles was about 1.42 μm. The corresponding EDS pattern in Figure 5f indicates that the material contains Lu, W, and O. After 5 mol%, Tb3+ was introduced in Lu2W3O12 (Figure 5g), and the morphology of the sample did not change significantly, and the average size of the particles was about 1.19 μm. The Tb element was also detected in addition to Lu, W, and O in the corresponding EDS pattern, as shown in Figure 5h. The FE-SEM images suggest that the Lu2Mo3O12 samples have bigger size particles than those Lu2W3O12 samples. Tb3+ doping did not lead to apparent changes in the particle morphologies nor in their the sizes. The EDS patterns proved the compositions of the samples. The Tb3+ doping did affect the PL properties greatly.

3.3. PL Properties

The preparation of temperature-dependent PL excitation spectra of Tb3+-doped Lu2W3O12 monitored at 5D47F5 emission are shown in Figure 6. With the preparation temperature increased from 800 °C to 1300 °C, all PL excitation spectra show broad excitation bands in the wavelength range of 200 nm to 330 nm, which can be attributed to the O2−-W6+ charge transfer band (CTB) transition from host [WO4]2− and the 4f–5d transition of Tb3+ [25,26]. The excitation intensities of CTB and 4f–5d transition of Tb3+ increased firstly, and reached the maxima at 1200 °C, and then decreased when the temperature increased to 1300 °C. The narrow weak excitation peaks in the wavelength range of 330 nm to 500 nm originated from the 4f–4f transition absorption of Tb3+. Comparing the samples prepared at 900 °C and higher temperatures, the 4f–4f transition absorptions of Tb3+ prepared at 800 °C were very weak, suggesting that the Tb3+ was not successfully doped into the host lattice. The phosphor prepared at 900 °C presented apparent Tb3+ 4f–4f transition absorptions. In addition, the intensities of CTB and 4f–5d of Tb3+ transitions were much stronger than those of the 4f–4f transition of Tb3+. The PL excitation spectra suggests that the optimum preparation temperature is 1200 °C for Tb3+-doped Lu2W3O12 phosphors.
Figure 7 shows the preparation of the temperature-dependent PL excitation spectra of Tb3+-doped Lu2Mo3O12. By monitoring the 5D47F5 emission at 547 nm, the PL excitation spectra of phosphor prepared at different preparation temperature shows a strong and broad excitation band in the wavelength range from 200 nm to 330 nm, which can be attributed to O2−-Mo6+ CTB transition from host [MoO4]2− at about 260 nm and the 4f–5d transition of Tb3+ located at about 282 nm. With the preparation temperature increasing, the relative CTB excitation intensities of the O2−-Mo6+ and 4f–5d transition of Tb3+ changed. The O2−-Mo6+ CTB was superior in the phosphors prepared at 800, 900, and 1000 °C, whereas for the phosphors prepared at 1100, 1200, and 1300 °C, the 4f–5d transition of Tb3+ prevailed. In addition, with the preparation temperature increased from 800 °C to 1300 °C, the excitation intensity of CTB increased firstly and then decreased, reaching the maxima at 1100 °C. For the excitation peaks originating from the 4f–4f transitions of Tb3+ located in the wavelength range of 330 nm to 500 nm, the intensities of the excitations increased with the calcine temperature increasing. Unlike the PL excitation intensities of Tb3+-doped Lu2W3O12, the intensities of CTB and the 4f–5d transitions of Tb3+ were similar to those of the 4f–4f transitions of Tb3+.
As is shown in Figure 7, the CTB excitation intensity of the Tb3+-doped Lu2Mo3O12 phosphors prepared at 1000 °C and 1100 °C were similar. Considering the principle of energy saving and the safety in lab, 1000 °C was selected as the preparation temperature to prepare and compare the Tb3+-doped Lu2Mo3O12 and Lu2W3O12 phosphors.
Figure 8 shows the PL excitation and emission spectra of 5 mol% Tb3+-doped Lu2W3O12 and Lu2Mo3O12 phosphors. By monitoring the 547 nm emission corresponding to the 5D47F5 transition of Tb3+, the PL excitation spectra are composed of two parts. One part is a strong and broad excitation band in the wavelength range of 200–330 nm. There is one peak located at about 260 nm, which is generated by the O2− (2p)–W6+ (5d) or O2− (2p)–Mo6+ (4d) CTB transition from host [WO4]2− or [MoO4]2− groups. In addition, there is a peak at about 275 nm (or 282 nm), which originates from the Tb3+ 4f–5d transition [25,26]. The existence of the CTBs and the spectral overlap of the excitation spectra suggest the energy transfer between the [WO4]2−or [MoO4]2− groups and Tb3+. In the wavelength of 330 nm to 500 nm, there are characteristic 4f–4f transitions of Tb3+ peaked at 321, 344, 354, 361, 372, and 380 nm, corresponding to the transitions of the 7F65D0, 7F65G2, 7F65D2, 7F65G5, 7F65G6, and 7F65D3 transitions [27], respectively. The strongest one peaked at 380 nm in the near-ultraviolet (NUV) region, which suggests that the Lu2W3O12 and Lu2Mo3O12 phosphors can be excited by NUV LED chips. For the Tb3+-doped Lu2W3O12 and Lu2Mo3O12 phosphors, with 260 nm and 380 nm excitation, four emission peaks at 492, 547, 586, and 622 nm originating from the 5D47F6, 5D47F5, 5D47F4, 5D47F3 transitions of Tb3+ are recorded. The 5D47F5 transition that peaked at 547 nm is the strongest emission, and the phosphors yielded a bright green light. The insets are the corresponding photographs captured under the illumination of 254 nm light in a camera obscura, which indicate the successful preparation of green phosphors.
Under 254 nm light, the Lu2W3O12 phosphor produced a stronger bright green light than that of the Lu2Mo3O12 phosphor seen by the naked eye. To confirm that, Figure 9 displays the PL excitation spectra of the two phosphors which were recorded under the same measurement conditions. By monitoring at 547 nm emission of the transition 5D47F5 of Tb3+, the Lu2W3O12 phosphor presented about 1.5 times the excitation intensity of CTBs and Tb3+ 4f–5d transitions than those of the Lu2Mo3O12 phosphor. Yet, the two phosphors illustrated the similar intensities of Tb3+ 4f–4f transitions. When the preparation temperature was 1000 °C, Lu2W3O12 phosphor was a better choice than Lu2Mo3O12 phosphor for CTB excitation.

3.4. DRS

The DRS of 5 mol% Tb3+-doped and undoped Lu2W3O12 and Lu2Mo3O12 materials are shown in Figure 10. All the materials have low reflectance in the wavelength range of 200–350 nm, which mean the materials have strong absorptions in the wavelength range. The absorptions can be attributed to the CTBs of O2−-W6+ or O2−-Mo6+ and Tb3+ 4f–5d transitions. As can be seen from Figure 10, the incorporation of Tb3+ caused the movements of the absorptions to short wavelength range. The energy gap value Eg of the materials can be estimated from DRS by using equation [28]:
( α h ν ) n = c ( h ν E g )
where α, h, υ, and c are the absorption coefficient, the Planck’s constant, the incident light frequency and a constant, respectively. The value of n is 2 or 1/2, depending on the transition mode of the material, and n = 2 is a direct transition, whereas n = 1/2 is an indirect transition. The absorption coefficient α can be solved by using the Kubelka–Munk equation [29]:
F ( R ) = ( 1 R ) 2 2 R = K S
In this function, the reflection coefficient R is recorded by DRS, S is the scattering coefficient and independent on the wavelength of the incident light, and the value of K is proportional to α in Equation (1). In this case, n equals 1/2 and Lu2W3O12 [30] and Lu2Mo3O12 [31] are both indirect bandgap materials. By plotting [F(R)]1/2 versus , the value of Eg can be obtained. The insert in Figure 10 presents the [F(R)]1/2- plots of undoped Lu2W3O12 and Lu2Mo3O12 samples. By extrapolating F(R) to 0, the values of Eg of 4.02 eV and 3.94 eV for undoped Lu2W3O12 and Lu2Mo3O12 samples were obtained, respectively. For 5 mol% Tb3+-doped Lu2W3O12 and Lu2Mo3O12 phosphors, the obtained values of Eg were 4.06 eV and 3.95 eV. The value Eg of the Lu2W3O12 material was larger than that of the Lu2Mo3O12 material, and the value Eg of the doped material was larger than that of corresponding undoped material. The wide band gap is good for luminescent materials [32].

3.5. Measuring Temperature Dependent Spectra, Activation Energy, and Decay Curves

Thermal stability is usually used to evaluate phosphors [33,34]. Figure 11 shows the measuring of temperature-dependent PL excitation spectra of Tb3+-doped Lu2Mo3O12 phosphors by monitoring at a 547 nm emission of Tb3+. With the measuring temperature increasing from 50 °C to 250 °C, all the intensities of the excitation peaks became weaker. Correspondingly, the emission intensity decreased as well. The thermal luminescence quenching is usually caused by non-radiative transitions at high working temperature [35,36]. At a normal working temperature about 150 °C, the Lu2Mo3O12 phosphor kept 86% and 76% intensity of that at 50 °C with 260 nm and 380 nm excitations, respectively. Put another way, the emission intensity reduces to 50% of the initial intensity defined as quenching temperature T0.5 [37]. In the Lu2Mo3O12 phosphor, the T0.5 is 215 °C and 192 °C with 260 nm and 380 nm excitations.
The activation energy (Ea) of the Lu2Mo3O12 phosphor was also evaluated by using the Arrhenius formula [38]:
I T = I 0 1 + c exp ( E a / k T )
where I0 is the initial emission intensity of Tb3+, IT is the emission intensity of Tb3+ at temperature T, c is the quenching frequency factor, and k is the Boltzmann constant and equals 8.617 × 10−5 eV/K [39]. Evolving the formular to ln[(I0/IT) − 1] = (−Ea/k)(1/T) + c1, plotting ln[(I0/IT) − 1] corresponding 1/T, and linear fitting, the −Ea/k can be determined. Further, the Ea value can be obtained. As shown in Figure 12, the data obtained at high temperatures of 220 °C and 250 °C decayed rapidly and the data were not used in the fitting procedure. The values of −Ea/k were −2340 and −4656 with 260 nm and 380 nm excitations, respectively. Correspondingly, the values of Ea were 0.202 eV and 0.401 eV with 260 nm and 380 nm excitations. The results suggest that the Tb3+-doped Lu2Mo3O12 phosphor has wonderful thermal stabilities.
Unlike the Tb3+-doped Lu2Mo3O12, the Tb3+-doped Lu2W3O12 presents a different thermal behavior. For clarity, the measuring temperature and the monitoring wavelength were placed in the temperature-axis with the front number representing the measuring temperature and the latter number representing the monitoring wavelength. As shown in Figure 13, with the measuring temperature increasing, the PL excitation intensity varied differently by monitoring at the 5D47F5 transition. The intensities of Tb3+ 4f–4f transitions always decreased with the temperature increasing from 50 °C to 300 °C. Yet, the intensity of the CTB transition decreased with the temperature increasing to 150 °C. When the temperature increased further, the CTB and the Tb3+ 4f–5d transitions increased suddenly at about 170 °C and were hardly unchanged, even when the temperature was increased to 300 °C. Furthermore, the peak wavelength of the 5D47F5 transition varied from 546 nm to 552 nm with the measuring temperature increasing. Similar phenomena have been reported in Eu3+-doped Lu2(MoO4)3 [22,23]. The enhancing luminescence of Eu3+ in Lu2(MoO4)3 was recorded at about 250 °C, yet the enhancing luminescence of Tb3+ in Lu2W3O12 was recorded at about 170 °C. The enhancing temperature was lowered to about 80 °C, which was closer to practical applications. The enhancing luminescence has a relationship with the NTE property of the Lu2W3O12 crystal lattice.
The fluorescent decay curves of the Tb3+-doped Lu2W3O12 and Lu2Mo3O12 phosphors by monitoring at 547 nm with 260 nm excitation are shown in Figure 14. The two decay curves can both be fitted by a single exponential function:
I ( t ) = I 0 exp ( t / τ ) + c
where I0, I(t), τ, and c are emission intensity at initial time, emission intensity at t time, the corresponding fluorescent lifetime, and the background or zero offset, respectively. The fitted lifetimes were 0.724 ms and 0.689 ms for the 5 mol% Tb3+-doped Lu2W3O12 and Lu2Mo3O12 phosphors, respectively. The results suggest that the lifetime corresponding to the 5D4 level of Tb3+ was longer in the Lu2W3O12 host lattice than in the Lu2Mo3O12 host lattice, which is similar to those reported.

4. Conclusions

In conclusion, by using a solid-state reaction method, the Tb3+-doped and undoped Lu2W3O12 and Lu2Mo3O12 materials were prepared under different calcine temperatures. The XRD results suggest that the 5 mol% Tb3+-doping did not cause apparent variations on the XRD patterns besides the diffraction intensities. The FE-SEM pictures and the particle size distribution statistics illustrate that the materials were all composed of micrometer particles and the Lu2W3O12 samples had smaller particles than that of the Lu2Mo3O12 samples. The EDS patterns confirmed the compositions of Lu, Mo or W, O, and/or Tb in the materials. The preparing of temperature-dependent PL excitation spectra suggested that the optimum preparation temperature was 1200 °C for Tb3+-doped Lu2W3O12 phosphors and 1100 °C for Tb3+-doped Lu2Mo3O12 phosphors, respectively. The Tb3+-doped Lu2Mo3O12 phosphors prepared at 1000 °C and 1100 °C presented equivalent CTB excitation intensities, and 1000 °C was selected as the calcine temperature to prepare and compare the Tb3+-doped and undoped Lu2Mo3O12 and Lu2W3O12 materials. The Tb3+-doped Lu2W3O12 green phosphor showed a stronger PL excitation intensity of CTB than that of the Tb3+-doped Lu2Mo3O12 green phosphor. For undoped and doped Lu2W3O12 and Lu2Mo3O12 materials, the values of Eg calculated from the DRS were 4.02, 4.06, 3.94, and 3.95 eV, respectively. The values of Eg of the Lu2W3O12 materials were larger than that of the Lu2Mo3O12 materials. The measuring temperature dependent spectra indicated that the values of activation energy Ea of the Tb3+-doped Lu2Mo3O12 phosphors were 0.202 eV and 0.401 eV with 260 nm and 380 nm excitation, respectively, whereas the Tb3+-doped Lu2W3O12 phosphor illustrated a thermal enhancing CTB excitation intensity at 170 °C. The PL decay curves suggested that the lifetime corresponding to the 5D4 level of Tb3+ was longer in the Lu2W3O12 host lattice than in the Lu2Mo3O12 host lattice. The Tb3+-doped Lu2W3O12 showed potential as an application in temperature sensors.

Author Contributions

Conceptualization, C.C. and A.X.; methodology, N.H., M.Z. and Z.C.; formal analysis, B.B., N.H., M.Z., Z.C. and C.C.; investigation, B.B., N.H., M.Z., Z.C. and C.C.; data curation, Y.L., B.B. and N.H.; writing—original draft preparation, N.H., G.L. and B.B.; writing—review and editing, G.L., Y.L. and C.C.; supervision, C.C., Y.L. and A.X.; project administration, C.C. and A.X.; funding acquisition, C.C. and A.X. All authors have read and agreed to the published version of the manuscript.

Funding

The research work was supported by the Natural Science Foundation of Fujian Province (Grant no. 2021J011207), the Open Fund of Fujian Provincial Key Laboratory of Functional Materials and Applications (Xiamen University of Technology fma2022006), the Key Project of Natural Science Foundation of Fujian Province (Grant no. 2020J02049), the Key Technical Innovation and Industrialization Projects of Fujian Province (Grant no. 2022G049), and the Major Project of Science and Technology of Xiamen City (Grant nos. 3502ZCQ20201001).

Institutional Review Board Statement

Not applicable.

Informed Consent Statement

Not applicable.

Data Availability Statement

Not applicable.

Conflicts of Interest

The authors declare no conflict of interest.

References

  1. Shi, S.K.; Li, K.Y.; Wang, S.P.; Zong, R.L.; Zhang, G.L. Structural characterization and enhanced luminescence of Eu-doped 2CeO2–0.5La2O3 composite phosphor powders by a facile solution combustion synthesis. J. Mater. Chem. C 2017, 5, 4302–4309. [Google Scholar] [CrossRef]
  2. Lu, J.F.; Mu, Z.F.; Zhu, D.Y.; Wang, Q.; Wu, F.G. Luminescence properties of Eu3+ doped La3Ga5GeO14 and effect of Bi3+ co-doping. J. Lumin. 2018, 196, 50–56. [Google Scholar] [CrossRef]
  3. Li, W.F.; Qiu, M.F.; Li, Y.X.; Zhang, S.A.; Li, Q.F.; Lin, W.X.; Mu, Z.F.; Wu, F.G. Energy Transfer and Multicolor-Tunable Emissions of Sr3La6(SiO4)6: Ce3+, Tb3+, Eu3+. J. Electron. Mater. 2020, 49, 1404–1411. [Google Scholar] [CrossRef]
  4. Mu, Z.F.; Hu, Y.H.; Chen, L.; Wang, X.J.; Ju, G.F.; Yang, Z.F.; Jin, Y.H. A single-phase, color-tunable, broadband-excited white light-emitting phosphor Y2WO6: Sm3+. J. Lumin. 2014, 146, 33–36. [Google Scholar] [CrossRef]
  5. Nair, G.B.; Swart, H.C.; Dhoble, S.J. A review on the advancements in phosphor-converted light emitting diodes (pc-LEDs): Phosphor synthesis, device fabrication and characterization. Prog. Mater. Sci. 2020, 109, 100622. [Google Scholar] [CrossRef]
  6. Liu, X.; Li, L.; Noh, H.M.; Moon, B.K.; Choi, B.C.; Jeong, J.H. Chemical bond properties and charge transfer bands of O2−-Eu3+, O2−-Mo6+ and O2−-W6+ in Eu3+-doped garnet hosts Ln3M5O12 and ABO4 molybdate and tungstate phosphors. Dalton Trans. 2014, 43, 8814–8825. [Google Scholar] [CrossRef]
  7. Li, H.Y.; Yang, H.K.; Moon, B.K.; Choi, B.C.; Jeon, J.H.; Jang, K.W.; Lee, H.S.; Yi, S.S. Crystal Structure, Electronic Structure, and Optical and Photoluminescence Properties of Eu(III) Ion-Doped Lu6Mo(W)O12. Inorg. Chem. 2011, 50, 12522–12530. [Google Scholar] [CrossRef]
  8. Lee, G.H.; Kim, T.H.; Yoon, C.; Kang, S. Effect of local environment and Sm3+-codoping on the luminescence properties in the Eu3+-doped potassium tungstate phosphor for white LEDS. J. Lumin. 2008, 128, 1922–1926. [Google Scholar] [CrossRef]
  9. Baur, F.; Jüstel, T. (INVITED) Eu3+ activated molybdates—Structure property relations. Opt. Mater. X 2019, 1, 100015. [Google Scholar] [CrossRef]
  10. Cao, C.Y.; Zhang, Z.J.; Wei, S.J.; Xie, A.; Noh, H.M.; Jeong, J.H. Synthesis, optical properties, energy transfer, thermal behavior, and LED package of Eu3+ doped lutetium tungsten oxide phosphors. Opt. Mater. 2020, 101, 109753. [Google Scholar] [CrossRef]
  11. Cao, C.Y.; Wei, S.J.; Zhu, Y.X.; Liu, T.; Xie, A.; Noh, H.M.; Jeong, J.H. Synthesis, optical properties, and packaging of Dy3+ doped Y2WO6, Y2W3O12, and Y6WO12 phosphors. Mater. Res. Bull. 2020, 126, 110846. [Google Scholar] [CrossRef]
  12. Yan, S.; Zhang, J.; Zhang, X.; Lu, S.; Ren, X.; Nie, Z.; Wang, X. Enhanced red emission in CaMoO4:Bi3+, Eu3+. J. Phys. Chem. C 2007, 111, 13256–13260. [Google Scholar] [CrossRef]
  13. Zhou, Y.; Yan, B. RE2(MO4)3: Ln3+(RE = Y, La, Gd, Lu; M = W, Mo; Ln = Eu, Sm, Dy) microcrystals: Controlled synthesis, microstructure and tunable luminescence. CrystEngComm 2013, 15, 5694–5702. [Google Scholar] [CrossRef]
  14. Li, L.; Shen, J.; Zhou, X.J.; Pan, Y.; Chang, W.X.; He, Q.W.; Wei, X.T. Luminescent properties of Lu2MoO6:Eu3+ red phosphor for solid state lighting. Trans. Nonferr. Met. Soc. China 2016, 26, 1670–1675. [Google Scholar] [CrossRef]
  15. Guan, L.; Wei, W.; Guo, S.Q.; Su, H.X.; Li, X.; Shang, Y.X.; Yang, Z.P.; Guo, Q.L.; Fu, G.S. Fabrication and Luminescent Properties of Tb3+ Doped Double Molybdate Phosphors. J. Electrochem. Soc. 2012, 159, D200–D203. [Google Scholar] [CrossRef]
  16. Mahlik, S.; Diaz, F.; Boutinaud, P. Luminescence quenching in KYb(WO4)2-Tb3+: An example of temperature-pressure equivalence. J. Lumin. 2017, 191, 18–21. [Google Scholar] [CrossRef]
  17. Chen, X.Y.; Zhang, Z.J.; Feng, A.; Xu, M.; Zhao, J.T.; Xu, F.F. Electronic structure, optical and thermal/concentration quenching properties of Lu2−2xEu2xWO6 (0 ≤ x ≤ 0.2). Mater. Res. Bull. 2015, 70, 26–31. [Google Scholar] [CrossRef]
  18. Dang, P.P.; Li, G.G.; Yun, X.H.; Zhang, Q.Q.; Liu, D.J.; Lian, H.Z.; Shang, M.M.; Lin, J. Thermally stable and highly efficient red-emitting Eu3+-doped Cs3GdGe3O9 phosphors for WLEDs: Non-concentration quenching and negative thermal expansion. Light Sci. Appl. 2021, 10, 29. [Google Scholar] [CrossRef] [PubMed]
  19. Geng, X.; Xie, Y.; Chen, S.S.; Luo, J.M.; Li, S.C.; Wang, T.; Zhao, S.C.; Wang, H.; Deng, B.; Yu, R.J.; et al. Enhanced local symmetry achieved zero-thermal-quenching luminescence characteristic in the Ca2InSbO6:Sm3+ phosphors for w-LEDs. Chem. Eng. J. 2021, 410, 128396. [Google Scholar] [CrossRef]
  20. Zou, H.; Yang, X.Q.; Chen, B.; Du, Y.Y.; Ren, B.Y.; Sun, X.Q.; Qiao, X.S.; Zhang, Q.W.; Wang, F. Thermal Enhancement of Upconversion by Negative Lattice Expansion in Orthorhombic Yb2W3O12. Angew. Chem. Int. Ed. 2019, 58, 17255–17259. [Google Scholar] [CrossRef]
  21. Zou, H.; Chen, B.; Hu, Y.F.; Zhang, Q.W.; Wang, X.S.; Wang, F. Simultaneous Enhancement and Modulation of Upconversion by Thermal Stimulation in Sc2Mo3O12 Crystals. J. Phys. Chem. Lett. 2020, 11, 3020–3024. [Google Scholar] [CrossRef] [PubMed]
  22. Cao, C.Y.; Xie, A.L.; Zhou, T.L.; Zhong, H.C.; Lu, X.J.; Xie, A.; Noh, H.M.; Jeong, J.H. Eu3+ doped lutetium molybdenum oxides: Synthesis, optical properties, thermal behavior, and LED packaging. J. Lumin. 2020, 217, 116759. [Google Scholar] [CrossRef]
  23. Chen, Z.J.; Cao, C.Y.; Zhang, M.; Huang, N.H.; Bai, B.H.; Yang, L.; Li, Y.C.; Xie, A. Thermal enhancing photoluminescence intensities of Eu3+ doped Lu2(MoO4)3. Opt. Mater. 2022, 127, 112301. [Google Scholar] [CrossRef]
  24. Sumithra, S.; Umarji, A.M. Negative thermal expansion in rare earth molybdates. Solid State Sci. 2006, 8, 1453–1458. [Google Scholar] [CrossRef]
  25. Nugent, L.J.; Baybarz, R.D.; Burnett, J.L.; Ryan, J.L. Electron-transfer and f-d absorption bands of some lanthanide and actinide complexes and the standard (II–III) oxidation potential for each member of the lanthanide and actinide series. J. Phys. Chem. C 1973, 77, 1528–1539. [Google Scholar] [CrossRef]
  26. Baur, F.; Glocker, F.; Jüstel, T. Photoluminescence and energy transfer rates and efficiencies in Eu3+ activated Tb2Mo3O12. J. Mater. Chem. C 2015, 3, 2054–2064. [Google Scholar] [CrossRef] [Green Version]
  27. Liu, Y.X.; Yue, X.J.; Cai, K.; Deng, H.D.; Zhang, M. Microwave-assist hydrothermal synthesis and luminescence of NaGd(WO4):Tb3+ phosphors: A case study for the energy saving in the synthesis of phosphors. Energy 2015, 93, 1413–1417. [Google Scholar] [CrossRef]
  28. Zeng, W.; Wang, Y.H.; Han, S.C.; Chen, W.B.; Li, G.; Wang, Y.Z.; Wen, Y. Design, synthesis and characterization of a novel yellow long-persistent phosphor: Ca2BO3Cl:Eu2+, Dy3+. J. Mater. Chem. C 2013, 17, 3004–3011. [Google Scholar] [CrossRef]
  29. Cao, G.; Rabenberg, L.; Nunn, C.M.; Mallouk, T.E. Formation of quantum-size semiconductor particles in a layered metal phosphonate host lattice. Chem. Mater. 1991, 3, 149–156. [Google Scholar] [CrossRef]
  30. Materials Project. Available online: https://materialsproject.org/materials/mp-768455?chemsys=Lu-W-O (accessed on 10 November 2021).
  31. Wang, B.; Li, X.S.; Zeng, Q.G.; Yang, G.T.; Luo, J.Y.; He, X.; Chen, Y.Q. Efficiently enhanced photoluminescence in Eu3+-doped Lu2(MoO4)3 by Gd3+ substituting. Mater. Res. Bull. 2018, 100, 97–101. [Google Scholar] [CrossRef]
  32. Zhang, M.; Cao, C.Y.; Zhang, C.L.; Chen, Z.J.; Bai, B.H.; Huang, N.H.; Xie, A. Synthesis and Luminescent Properties of Gd2[1-x(y)]Eu2x(y)WzMo(1-z)O6 Red Phosphors. Chin. J. Lumin. 2022, 43, 1086–1094. [Google Scholar] [CrossRef]
  33. Ueda, J.; Dorenbos, P.; Bos, A.J.J.; Meijerink, A.; Tanabe, S. Insight into the Thermal Quenching Mechanism for Y3Al5O12:Ce3+ through Thermoluminescence Excitation Spectroscopy. J. Phys. Chem. C 2015, 119, 25003–25008. [Google Scholar] [CrossRef] [Green Version]
  34. Kim, Y.H.; Arunkumar, P.; Kim, B.Y.; Unithrattil, S.; Kim, E.; Moon, S.H.; Hyun, J.Y.; Kim, K.H.; Lee, D.; Lee, J.S.; et al. A Zero-thermal-quenching Phosphor. Nat. Mater. 2017, 16, 543–550. [Google Scholar] [CrossRef] [PubMed]
  35. Xu, S.C.; Wang, Z.J.; Li, P.L.; Li, T.; Bai, Q.Y.; Sun, J.; Yang, Z.P. Single-phase white-emitting phosphors Ba3Ce(1-x-y)(PO4)3:xTb3+,yMn2+ and Ba3Ce(1-x-z)(PO4)3:xTb3+,zSm3+: Structure, luminescence, energy transfer and thermal stability. RSC Adv. 2017, 7, 19584–19592. [Google Scholar] [CrossRef] [Green Version]
  36. Tian, M.M.; Li, P.L.; Wang, Z.J.; Teng, X.Y.; Li, Z.L.; Cheng, J.G.; Sun, Y.S.; Wang, C.; Yang, Z.P. Synthesis, color-tunable emission, thermal stability, luminescence and energy transfer of Sm3+ and Eu3+ single-doped M3Tb(BO3)3 (M = Sr and Ba) phosphors. CrystEngComm 2016, 18, 6934–6947. [Google Scholar] [CrossRef]
  37. Wang, Y.; Deng, B.; Ke, Y.; Shu, S.; Liu, R.X.; Yu, R.J. Spectroscopic investigation of La7Ta3W4O30:Sm3+ orange-red phosphor for white LEDs. Arab. J. Chem. 2020, 13, 5581–5592. [Google Scholar] [CrossRef]
  38. Bhushan, S.; Chukichev, M.V. Temperature dependent studies of cathodoluminescence of green band of ZnO crystals. J. Mater. Sci. Lett. 1988, 7, 319–321. [Google Scholar] [CrossRef]
  39. Qiao, J.; Zhang, Z.C.; Zhao, J.; Xia, Z.G. Tuning of the Compositions and Multiple Activator Sites toward Single-Phased White Emission in (Ca9–xSrx)MgK(PO4)7:Eu2+ Phosphors for Solid-State Lighting. Inorg. Chem. 2019, 58, 5006–5012. [Google Scholar] [CrossRef]
Figure 1. Preparation of temperature-dependent XRD patterns of Tb3+-doped Lu2W3O12 and reference data.
Figure 1. Preparation of temperature-dependent XRD patterns of Tb3+-doped Lu2W3O12 and reference data.
Chemosensors 10 00533 g001
Figure 2. Preparation of temperature-dependent XRD patterns of Tb3+-doped Lu2Mo3O12 and reference data.
Figure 2. Preparation of temperature-dependent XRD patterns of Tb3+-doped Lu2Mo3O12 and reference data.
Chemosensors 10 00533 g002
Figure 3. XRD patterns of 5 mol%Tb3+-doped and undoped Lu2W3O12 and Lu2Mo3O12 materials prepared at 1000 °C and reference data.
Figure 3. XRD patterns of 5 mol%Tb3+-doped and undoped Lu2W3O12 and Lu2Mo3O12 materials prepared at 1000 °C and reference data.
Chemosensors 10 00533 g003
Figure 4. Schematic crystal structure diagrams of Lu2W3O12 (a) and Lu2Mo3O12 (b).
Figure 4. Schematic crystal structure diagrams of Lu2W3O12 (a) and Lu2Mo3O12 (b).
Chemosensors 10 00533 g004
Figure 5. FE-SEM images and EDS spectra of undoped Lu2Mo3O12 (a,b), 5 mol% Tb3+-doped Lu2Mo3O12 (c,d), undoped Lu2W3O12 (e,f), and 5 mol% Tb3+-doped Lu2W3O12 (g,h) prepared at 1000 °C. Insets in FE-SEM images are corresponding particle size distribution statistics.
Figure 5. FE-SEM images and EDS spectra of undoped Lu2Mo3O12 (a,b), 5 mol% Tb3+-doped Lu2Mo3O12 (c,d), undoped Lu2W3O12 (e,f), and 5 mol% Tb3+-doped Lu2W3O12 (g,h) prepared at 1000 °C. Insets in FE-SEM images are corresponding particle size distribution statistics.
Chemosensors 10 00533 g005
Figure 6. Preparation of temperature-dependent PL excitation spectra of Tb3+-doped Lu2W3O12 phosphors.
Figure 6. Preparation of temperature-dependent PL excitation spectra of Tb3+-doped Lu2W3O12 phosphors.
Chemosensors 10 00533 g006
Figure 7. Preparation of temperature-dependent PL excitation spectra of Tb3+-doped Lu2Mo3O12 phosphors.
Figure 7. Preparation of temperature-dependent PL excitation spectra of Tb3+-doped Lu2Mo3O12 phosphors.
Chemosensors 10 00533 g007
Figure 8. PL excitation and emission spectra of 5 mol%Tb3+-doped Lu2W3O12 and Lu2Mo3O12 phosphors prepared at 1000 °C. Inserts are the corresponding phosphor pictures captured under 254 nm light.
Figure 8. PL excitation and emission spectra of 5 mol%Tb3+-doped Lu2W3O12 and Lu2Mo3O12 phosphors prepared at 1000 °C. Inserts are the corresponding phosphor pictures captured under 254 nm light.
Chemosensors 10 00533 g008
Figure 9. Comparison of PL excitation spectra of 5 mol% Tb3+-doped Lu2W3O12 and Lu2Mo3O12 phosphors prepared at 1000 °C.
Figure 9. Comparison of PL excitation spectra of 5 mol% Tb3+-doped Lu2W3O12 and Lu2Mo3O12 phosphors prepared at 1000 °C.
Chemosensors 10 00533 g009
Figure 10. DRS of 5 mol% Tb3+-doped and undoped Lu2W3O12 and Lu2Mo3O12 materials. Inserts display [F(R)hν]1/2-hν plots of undoped Lu2W3O12 and Lu2Mo3O12 samples prepared at 1000 °C.
Figure 10. DRS of 5 mol% Tb3+-doped and undoped Lu2W3O12 and Lu2Mo3O12 materials. Inserts display [F(R)hν]1/2-hν plots of undoped Lu2W3O12 and Lu2Mo3O12 samples prepared at 1000 °C.
Chemosensors 10 00533 g010
Figure 11. Measuring of temperature-dependent PL excitation spectra of Tb3+-doped Lu2Mo3O12 phosphor prepared at 1000 °C.
Figure 11. Measuring of temperature-dependent PL excitation spectra of Tb3+-doped Lu2Mo3O12 phosphor prepared at 1000 °C.
Chemosensors 10 00533 g011
Figure 12. Plots of ln[(I0/IT)1] corresponding to 1/T in Tb3+-doped Lu2Mo3O12 phosphor prepared at 1000 °C.
Figure 12. Plots of ln[(I0/IT)1] corresponding to 1/T in Tb3+-doped Lu2Mo3O12 phosphor prepared at 1000 °C.
Chemosensors 10 00533 g012
Figure 13. Measuring temperature-dependent PL excitation spectra of Tb3+-doped Lu2W3O12 prepared at 1000 °C.
Figure 13. Measuring temperature-dependent PL excitation spectra of Tb3+-doped Lu2W3O12 prepared at 1000 °C.
Chemosensors 10 00533 g013
Figure 14. PL decay curves of Tb3+-doped Lu2W3O12 and Lu2Mo3O12 phosphors prepared at 1000 °C.
Figure 14. PL decay curves of Tb3+-doped Lu2W3O12 and Lu2Mo3O12 phosphors prepared at 1000 °C.
Chemosensors 10 00533 g014
Publisher’s Note: MDPI stays neutral with regard to jurisdictional claims in published maps and institutional affiliations.

Share and Cite

MDPI and ACS Style

Huang, N.; Lu, G.; Bai, B.; Chen, Z.; Zhang, M.; Li, Y.; Cao, C.; Xie, A. Preparation and Photoluminescent Properties of Tb3+-Doped Lu2W3O12 and Lu2Mo3O12 Green Phosphors. Chemosensors 2022, 10, 533. https://doi.org/10.3390/chemosensors10120533

AMA Style

Huang N, Lu G, Bai B, Chen Z, Zhang M, Li Y, Cao C, Xie A. Preparation and Photoluminescent Properties of Tb3+-Doped Lu2W3O12 and Lu2Mo3O12 Green Phosphors. Chemosensors. 2022; 10(12):533. https://doi.org/10.3390/chemosensors10120533

Chicago/Turabian Style

Huang, Nihui, Guojun Lu, Bihai Bai, Zijun Chen, Min Zhang, Yuechan Li, Chunyan Cao, and An Xie. 2022. "Preparation and Photoluminescent Properties of Tb3+-Doped Lu2W3O12 and Lu2Mo3O12 Green Phosphors" Chemosensors 10, no. 12: 533. https://doi.org/10.3390/chemosensors10120533

Note that from the first issue of 2016, this journal uses article numbers instead of page numbers. See further details here.

Article Metrics

Back to TopTop