Communication

Controlled Synthesis of Mg-MOF-74 and Its CO2 Adsorption in Flue Gas

Department of Chemistry and Chemical & Environmental Engineering, Weifang University, Weifang 261061, China
*
Authors to whom correspondence should be addressed.
Coatings 2024, 14(4), 383; https://doi.org/10.3390/coatings14040383
Submission received: 27 February 2024 / Revised: 20 March 2024 / Accepted: 21 March 2024 / Published: 25 March 2024
(This article belongs to the Section Environmental Aspects in Colloid and Interface Science)

Abstract

:
Yellow nanorod Mg-MOF-74 was obtained through a solvothermal synthesis method. The XRD, N2 adsorption–desorption isotherms, SEM, and TGA results suggest that the particle size of Mg-MOF-74 reaches 400 nm after the introduction of sodium acetate in the precursor of Mg-MOF-74. Furthermore, the morphology of Mg-MOF-74 changed from cauliflower- to rod-shaped particles. At the same time, the BET specific surface area and pore volume of Mg-MOF-74 also increased a lot. Then, the CO2 dynamic adsorption capacity of Mg-MOF-74 was measured with a self-made fixed bed at 30 °C and a 0.1 bar CO2 partial pressure. The results show that the CO2 adsorption capacity of Mg-MOF-74-N2 reaches 3.67 mmol/g, and its CO2 adsorption capacity remains unchanged after 10 CO2 adsorption–desorption cycles.

1. Introduction

Excessive CO2 emissions caused by the burning of fossil fuels and human activities have led to increasing global warming, melting glaciers, frequent climate disasters, and a sharp decline in plant and animal diversity. The United Nations (IPCC) has issued a goal of reducing global CO2 emissions by 41% by 2050 compared with 2010 [1]. In China, power plants are a concentrated source of CO2 emissions, accounting for 40% of the total CO2 emissions. Controlling CO2 emissions in the flue gas of power plants is the key to achieving CO2 emission reduction goals. At present, CO2 capture and storage (CCS) technology is a key technology for mitigating and controlling CO2 emissions, and reducing the cost of the capture stage is the top priority in implementing this technology. Based on the low CO2 content in the flue gas of power plants, the commonly used CO2 capture methods include absorption, adsorption, membrane separation, and low-temperature distillation. Among them, the adsorption method has the advantages of being a simple process, having mild operating conditions and low energy consumption, and incurring no corrosion to equipment, so it is the most promising capture method at present. At present, the most commonly used materials in the field of CO2 adsorption are activated carbon, molecular sieves, metal oxides, and metal-organic frameworks (MOFs) [2,3,4,5]. A high CO2 adsorption capacity, a fast absorption/desorption rate, good selectivity, good adsorption stability, and low regenerative energy consumption are the conditions for the preparation of excellent CO2 adsorbents. MOFs are a new type of crystalline porous material composed of metal ions and organic ligands [6]. The high specific surface area, developed porosity and tunable chemical composition characters make MOFs widely used in gas adsorption and separation [7,8,9,10,11], drug carrier [12], catalysis [13], sensors [7,14], and other fields. With the development of nanotechnology, nanoscale MOFs have attracted the attention of scientists because of their special morphology, particle size, and other excellent characteristics. At present, the synthesis methods of nanometer MOFs include the direct precipitation method, the microwave-assisted method, the hydrothermal/solvothermal synthesis method, the mechanical method, and so on.
For example, Ahn, et al. [15] reported a method for the preparation of nanoscale Mg-MOF-74 using ultrasonic chemistry, which uses triethylamine as the deprotonation agent and greatly reduces the reaction time. Sun’s [16] research group used polyethylpyrrolidone and ammonia water to regulate the morphology and particle size of Mg-MOF-74. In addition, the N2 adsorption and desorption results also show that the morphology and particle size of Mg-MOF-74 affect the adsorption properties of the gas. Chen’s [12] research group prepared Mg-MOF-74 with a particle size of less than 200 nm through a two-step method and explored its application as a drug carrier. Zhang [17] et al. reported that a Mg-MOF-74/sodium alginate composite aerogel was prepared by loading Mg-MOF-74 on sodium alginate sheets, followed by directional freeze-drying. The experimental data showed that the composite achieved a CO2 adsorption of 2.461 mmol/g at 298 K. This may be due to the hierarchical pore structure formed by the composite aerogel. The micropore/mesopore structure of Mg-MOF-74 can improve the interaction between CO2 and the adsorbent and enhance the gas mass transfer rate [1,18,19]. However, there are still few studies on CO2 adsorption of nanosized Mg-MOF-74 in flue gas.
In this paper, nanorod Mg-MOF-74 particles were synthesized by a simple solvothermal method without surfactants. The morphology and particle size of the MOFs were adjusted by controlling the concentration of sodium acetate (NaAc). The dynamic adsorption performance of nanoscale Mg-MOF-74 under a simulated flue gas environment was tested by a self-made fixed bed, which provided a theoretical basis for the design and synthesis of a CO2 adsorbent suitable for a power plant flue gas environment.

2. Experimental Part

2.1. Reagents and Characterization

2,5-dihydroxyterephthalic acid (H4DOBDC), magnesium nitrate hexahydrate (Mg(NO3)2·6H2O), N,N-dimethylformamide (DMF), anhydrous methanol (CH3OH), and sodium acetate (NaAc) were bought from Shanghai Aladdin Reagent Co., Ltd. (No. 809, Chuhua Branch Road, Fengxian District, Shanghai). The reagents used were all analytically pure. CO2 (high purity) was obtained from Beijing Beiwen Gas Factory, and N2 (high purity) was obtained from TISCO Gas Factory.
An X-ray diffraction analysis was performed with a D8 Advance X-ray diffractometer from Nikaku (Rigaku Corporation, Woodlands, TX, USA) using Cu Kα radiation (λ = 0.154 nm), a metal Ni filter, a tube pressure of 40 kV, and a tube flow of 30 mA. The N2 adsorption and desorption isotherms of the sample at 77 K were determined with an ASAP 2020 automatic physical adsorption instrument (Micromeritics, Norcross, GA, USA). The sample was vacuumed and degassed at 200 °C for one night before the test. The microstructure and morphology of the sample were observed using a JSM-7001 thermal field emission scanning electron microscope (JEOL Ltd., Tokyo, Japan). The sample was coated with a conductive adhesive and scanned after gold spraying. During the test, the acceleration voltage was 5–10 kV. A Rigaku TG thermogravimetric analyzer (Rigaku Corporation, Woodlands, TX, USA) was used to study the thermal stability of the sample. Under an N2 inert atmosphere, the weight of the sample was 10 mg. The thermogravimetric curve of the sample was tested in the range of 25–600 °C, and the heating rate was 10 °C/min.

2.2. Synthesis of Mg-MOF-74

H4DOBDC (0.674 g, 3.4 mmol) and Mg(NO3)2·6H2O (2.8 g, 10.9 mmol) were added to 300 mL of a DMF/EtOH/H2O mixed solution with a volume ratio of 15:1:1 and stirred until dissolved. Then, 0–2 equivalent amounts of NaAc were added to the mixture, and then the reaction liquid was placed in a crystallization kettle and reacted in an oven at 125 °C for 20 h. Finally, the mother liquid was poured out to obtain yellow microcrystals. The obtained crystals were impregnated into methanol solution for replacement once every two days for three consecutive times, and the crystals were washed with N, N-dimethylformamide (DMF) three times and then placed in a 200 °C vacuum-drying oven to remove the solvent and obtain Mg-MOF-74. The resulting sample is named Mg-MOF-74-N(0-2), where N represents NaAc and 0–2 represents the equivalent amount added to NaAc.

2.3. Evaluation of Adsorbents

The CO2 dynamic adsorption breakthrough experiment of the adsorbents were carried out on a self-made fixed bed. An appropriate amount of adsorbent was pressed through the screen, and 20–40 mg of adsorbent was put into a U-shaped quartz tube with an inner diameter of 5 mm. The adsorbent was activated in an Ar atmosphere at 200 °C for 6 h with a gas volume flow rate of 60 mL/min and a constant inlet concentration. The sample temperature dropped to the required temperature and maintained it during the CO2 adsorption process after activation. Switch the gas valve of CO2 and N2 (CO2/N2-1:9) and adjust the gas flow. Gas chromatography was used to detect the concentration of the air outlet every 10 s until the CO2 concentration of the air outlet was the same as the concentration of the air inlet, which suggests the adsorption process is over. The CO2 desorption experiment was carried out at a high temperature in an argon atmosphere. After desorption, the temperature was lowered to the specified adsorption temperature, and then the CO2 adsorption experiment was carried out.
According to the concentration of CO2 at the air outlet, the CO2 penetration curve of the material can be obtained, and the CO2 adsorption capacity can be calculated according to the penetration curve. The specific calculation formula is as follows:
q = Q t s t 0 C i n 22.4 W
t s = 0 t 1 C o u t C i n d t
where ts(s) is the average residence and adsorption time, t0(s) is the average residence and adsorption time of the empty bed, Cin and Cout are the CO2 concentrations of the import and export, respectively, that is, the volume fraction of CO2 in the gas, q is the CO2 equilibrium adsorption capacity of the material (mmol/g), and Q is the volume flow rate of the mixture (mL/s). W is the mass of the adsorbent.

3. Results and Discussion

To investigate the effect of the NaAc concentration on the structure of Mg-MOF-74, 0–2 equivalent amounts of NaAc were added to the precursor solution of Mg-MOF-74, and the resulting products were named Mg-MOF-74-N0, Mg-MOF-74-N0.5, Mg-MOF-74-N1, and Mg-MOF-74-N2, respectively. The obtained samples were characterized by XRD, and the results are shown in Figure 1. It can be seen from Figure 1 that the XRD diffraction peak of the samples is consistent with the XRD pattern reported in the literature [20]. After adding NaAc, the diffraction peak of Mg-MOF-74 did not change, indicating that the introduction of NaAc did not destroy the crystal structure. However, after adding NaAc, the diffraction peak intensity decreased rapidly, and with the increase in NaAc concentration, the diffraction peak intensity decreased gradually. The results showed that the crystallinity of the crystals decreased after the introduction of NaAc into the precursor solution of Mg-MOF-74.
To further investigate the effect of the NaAc concentration on the crystal morphology of Mg-MOF-74, the samples were characterized by SEM. As can be seen from Figure 2, without adding NaAc, the obtained Mg-MOF-74 showed the morphology of a cauliflower, consisting of rod-like particles aggregated into a cauliflower shape, which was consistent with the literature reports. The particle size of Mg-MOF-74-N0 was about 17 μm, and the size of the cauliflower particles was decreased to 13 μm after adding 0.5 equivalent amounts of NaAc. When the concentration of NaAc increased to 1 equivalent, Mg-MOF-74-N1 mainly presented rod-like particles, and the length and the diameter of rod particles were 5 μm and 1 μm. When the concentration of NaAc was further increased to two equivalent amounts, the obtained Mg-MOF-74-N2 still had rod-like particles with a diameter of about 3μm and a uniform distribution, and the diameter of the particles was about 400 nm. With the increase in NaAc concentration, the particle size of Mg-MOF-74 decreased from microns to nanometers.
To further test the pore structure properties of nanoscale Mg-MOF-74, N2 adsorption and desorption experiments were performed on the sample, and the results are shown in Figure 3. It can be seen from the N2 adsorption and desorption isotherms of the sample that the adsorption isotherm of Mg-MOF-74 synthesized without adding NaAc conforms to a type I adsorption isotherm, indicating that the pores in Mg-MOF-74 are micropores. The H3 hysteresis ring in the adsorption isotherm of Mg-MOF-74-N2 indicates the presence of mesoporous pores in the sample. This may be due to a reduction in the size of the crystals, resulting in the accumulation of holes. The pore volume, specific surface area, and pore diameter of Mg-MOF-74 and Mg-MOF-74-N2 are listed in Table 1. It can be seen from the data in the table that the pore volume increases with the increase in the specific surface area of Mg-MOF-74-N2, and the pore size remains almost unchanged. This shows that the addition of NaAc helps to increase the specific surface area of the crystal, and the increase in pore volume is due to the formation of many accumulation holes due to the reduction in crystal size, which leads to an increase in the total pore volume of the sample [21].
To further test the thermal stability of the Mg-MOF-74 crystal, we performed a thermogravimetric analysis of the sample, and the results are shown in Figure 4. The weight loss from room temperature to 100 °C is attributed to the moisture adsorbed in the Mg-MOF-74 hole, and the weight loss from 100 to 250 °C is attributed to the solvent adsorbed in the hole [22]. It can be seen from the thermogravimetric curve that the weight of Mg-MOF-74-N2 no longer decreases at 500 °C, while Mg-MOF-74 continues to lose weight at 600 °C, so the thermal stability of Mg-MOF-74-N2 is reduced compared with Mg-MOF-74.
A self-made fixed bed was used to test the dynamic CO2 adsorption performance of nanoscale Mg-MOF-74 in the simulated flue gas environment, and the dynamic adsorption penetration curve is shown in Figure 5. According to Formulas (1) and (2), the dynamic CO2 adsorption capacity of Mg-MOF-74-N2 under 30 °C and a 0.1 bar CO2 partial pressure is 3.63 mmol/g, which is much higher than the 1.62 mmol/g absorption capacity of Mg-MOF-74-N0 under the same conditions. This may be due to the increase in the specific surface area and pore volume of the synthesized Mg-MOF-74-N2 nanoparticles after the addition of NaAc, so their CO2 adsorption performance is also improved.
To test the regeneration performance of Mg-MOF-74-N2, we used a fixed bed to carry out the CO2 cycling absorption and desorption experiments on the adsorbent at 30 °C and a 0.1 bar CO2 partial pressure, and the results are shown in Figure 6. When the CO2 adsorption is saturated, the temperature rises to 200 °C for desorption under an Ar gas atmosphere, and then the temperature drops to 30 °C for CO2 adsorption under a 0.1 bar CO2 partial pressure. After 10 cycles of adsorption and desorption, the CO2 adsorption capacity of the adsorbent under 30 °C and a 0.1 bar CO2 partial pressure almost remains unchanged. The results indicated that the regeneration performance of Mg-MOF-74-N2 was high.

4. Conclusions

Mg-MOF-74 was synthesized through a solvothermal synthesis method. After adding NaAc to the precursor solution, the crystal morphology changed from cauliflower-type to rod-like particles, and the particle size changed from micron to nanometer particles. The dynamic CO2 adsorption performance of Mg-MOF-74 in a simulated flue gas environment was tested. The results showed that the CO2 adsorption performance of nanoscale MG-MOF-74-N2 synthesized by adding NaAc was significantly improved, and the CO2 adsorption capacity reached 3.63 mmol/g at 30 °C and a 0.1 bar CO2 partial pressure.

Supplementary Materials

The following supporting information can be downloaded at: https://www.mdpi.com/article/10.3390/coatings14040383/s1, Figure S1. XRD pattern of Mg-MOF-74 synthesized by adding different concentrations of NaAc. Figure S2. The PXRD spectra of Mg-MOF-74-N2 and NaAc. Figure S3. FTIR spectrum of Mg-MOF-74-N2 before and after washing with DMF.

Author Contributions

Writing—original draft preparation, C.X.; Data curation, S.H.; Formal analysis, L.Y.; Methodology, X.Z.; Resources, Y.F.; Writing—Validation, X.Y. and W.S.; Writing—rivew & editing, F.Y.; Project administration and methodology, X.W.; Funding acquisition, Resources and Conceptualization, L.L. All authors have read and agreed to the published version of the manuscript.

Funding

This research was funded by Xia Wang grant number (22108208) and The APC was funded by the National Natural Science Foundation of China (22108208).

Data Availability Statement

Data are contained within the article and supplementary materials.

Conflicts of Interest

The authors declare no conflict of interest.

References

  1. Xin, C.L.; Ren, Y.; Zhang, Z.F.; Liu, L.L.; Wang, X.; Yang, J.M. Enhancement of Hydrothermal Stability and CO2 Adsorption of Mg-MOF-74/MCF Composites. ACS Omega 2021, 6, 7739–7745. [Google Scholar] [CrossRef] [PubMed]
  2. Choi, S.; Drese, J.H.; Jones, C.W. Adsorbent Materials for Carbon Dioxide Capture from Large Anthropogenic Point Sources. ChemSusChem 2009, 2, 796–854. [Google Scholar] [CrossRef] [PubMed]
  3. Li, W.; Bollini, P.; Didas, S.A.; Choi, S.; Drese, J.H.; Jones, C.W. Structural Changes of Silica Mesocellular Foam Supported Amine-Functionalized CO2 Adsorbents Upon Exposure to Steam. ACS Appl. Mater. Interfaces 2010, 2, 3363–3372. [Google Scholar] [CrossRef]
  4. Comotti, A.; Fraccarollo, A.; Bracco, S.; Beretta, M.; Distefano, G.; Cossi, M.; Marchese, L.; Riccardi, C.; Sozzani, P. Porous dipeptide crystals as selective CO2 adsorbents: Experimental isotherms vs. grand canonical Monte Carlo simulations and MAS NMR spectroscopy. Crystengcomm 2013, 15, 1503–1507. [Google Scholar] [CrossRef]
  5. Halabi, M.H.; de Croon, M.H.J.M.; van der Schaaf, J.; Cobden, P.D.; Schouten, J.C. Kinetic and structural requirements for a CO2 adsorbent in sorption enhanced catalytic reforming of methane—Part I: Reaction kinetics and sorbent capacity. Fuel 2012, 99, 154–164. [Google Scholar] [CrossRef]
  6. Chui, S.S. A Chemically Functionalizable Nanoporous Material [Cu3(TMA)2(H2O)3]n. Science 1999, 283, 1148–1150. [Google Scholar] [CrossRef] [PubMed]
  7. Thomas, S.; Mayr, F.; Gagliardi, A. Adsorption and sensing properties of SF6 decomposed gases on Mg-MOF-74. Solid State Commun. 2023, 363, 115120–115124. [Google Scholar] [CrossRef]
  8. Yang, R.H.; Ullah, S.; Chen, X.; Ma, J.X.; Gao, Y.; Wang, Y.J.; Luo, G.S. Selective adsorption of liquid long-chain α-olefin/paraffin on Mg-MOF-74: Adsorption behavior and interaction mechanism. Nano Res. 2023, 16, 1595–1605. [Google Scholar] [CrossRef]
  9. Mallick, A.; Mouchaham, G.; Bhatt, P.M.; Liang, W.; Belmabkhout, Y.; Adil, K.; Jamal, A.; Eddaoudi, M. Advances in Shaping of Metal–Organic Frameworks for CO2 Capture: Understanding the Effect of Rubbery and Glassy Polymeric Binders. Ind. Eng. Chem. Res. 2018, 57, 16897–16902. [Google Scholar] [CrossRef]
  10. Alezi, D.; Belmabkhout, Y.; Suyetin, M.; Bhatt, P.M.; Weselinski, L.J.; Solovyeva, V.; Adil, K.; Spanopoulos, I.; Trikalitis, P.N.; Emwas, A.H.; et al. MOF Crystal Chemistry Paving the Way to Gas Storage Needs: Aluminum-Based soc-MOF for CH4, O2, and CO2 Storage. J. Am. Chem. Soc. 2015, 137, 13308–13318. [Google Scholar] [CrossRef]
  11. CREAMER, A.E.; Gao, B. Carbon-Based Adsorbents for Postcombustion CO2 Capture: A Critical Review. Environ. Sci. Technol. 2016, 50, 7276–7289. [Google Scholar] [CrossRef]
  12. Hu, J.Q.; Chen, Y.; Zhang, H.; Chen, Z.X. Controlled syntheses of Mg-MOF-74 nanorods for drug delivery. J. Solid State Chem. 2021, 294, 121853. [Google Scholar] [CrossRef]
  13. Chen, C.; Li, B.X.; Zhou, L.J.; Xia, Z.F.; Feng, N.J.; Ding, J.; Wang, L.; Wan, H.; Guan, G.F. Synthesis of Hierarchically Structured Hybrid Materials by Controlled Self-Assembly of Metal Organic Framework with Mesoporous Silica for CO2 Adsorption. ACS Appl. Mater. Interfaces 2017, 9, 23060–23071. [Google Scholar] [CrossRef]
  14. Yu, C.P.; Cui, J.W.; Wang, Y.; Zheng, H.M.; Zhang, J.F.; Shu, X.; Liu, J.Q.; Zhang, Y.; Wu, Y.C. Porous HKUST-1 derived CuO/Cu2O shell wrapped Cu(OH)2 derived CuO/Cu2O core nanowire arrays for electrochemical nonenzymatic glucose sensors with ultrahigh sensitivity. Appl. Surf. Sci. 2018, 439, 11–17. [Google Scholar] [CrossRef]
  15. Yang, D.A.; Cho, H.Y.; Kim, J.; Yang, S.T.; Ahn, W.S. CO2 capture and conversion using Mg-MOF-74 prepared by a sonochemical method. Energy Environ. Sci. 2012, 5, 6465. [Google Scholar] [CrossRef]
  16. Yao, Z.Y.; Guo, J.H.; Wang, P.; Liu, Y.; Guo, F.; Sun, W.Y. Controlled synthesis of micro/nanoscale Mg-MOF-74 materials and their adsorption property. Mater. Lett. 2018, 223, 174–177. [Google Scholar] [CrossRef]
  17. Peng, X.Q.; Zhang, J.; Sun, J.Q.; Liu, X.C.; Zhao, X.F.; Yu, S.M.; Yuan, Z.P.; Liu, S.J.; Yi, X.B. Hierarchically Porous Mg-MOF-74/Sodium Alginate Composite Aerogel for CO2 Capture. ACS Appl. Nano Mater. 2023, 6, 16694–16701. [Google Scholar] [CrossRef]
  18. Xin, C.; Zhan, H.; Huang, X.; Li, H.; Zhao, N.; Xiao, F.; Wei, W.; Sun, Y. Effect of various alkaline agents on the size and morphology of nano-sized HKUST-1 for CO2 adsorption. RSC Adv. 2015, 5, 27901–27911. [Google Scholar] [CrossRef]
  19. Xin, C.; Jiao, X.; Yin, Y.; Zhan, H.; Li, H.; Li, L.; Zhao, N.; Xiao, F.; Wei, W. Enhanced CO2 Adsorption Capacity and Hydrothermal Stability of HKUST-1 via Introduction of Siliceous Mesocellular Foams (MCFs). Ind. Eng. Chem. Res. 2016, 55, 7950–7957. [Google Scholar] [CrossRef]
  20. Chakraborty, A.; Maji, T.K. Mg-MOF-74@SBA-15 hybrids: Synthesis, characterization, and adsorption properties. APL Mater. 2014, 2, 124107–124113. [Google Scholar] [CrossRef]
  21. Li, F.F.; Chen, Y.N.; Gong, M.; Chen, A.J.; Li, L.; Zhang, Z.T.; Liu, Y.; Dan, N.H.; Li, Z.J. Core-shell structure Mg-MOF-74@MSiO2 with mesoporous silica shell having efficiently sustained release ability of magnesium ions potential for bone repair application. J. Non-Cryst. Solids 2023, 600, 122018. [Google Scholar] [CrossRef]
  22. An, H.F.; Tian, W.J.; Lu, X.; Yuan, H.M.; Yang, L.Y.; Zhang, H.; Shen, H.M.; Bai, H. Boosting the CO2 adsorption performance by defect-rich hierarchical porous Mg-MOF-74. Chem. Eng. J. 2023, 469, 144052. [Google Scholar] [CrossRef]
Figure 1. XRD pattern of Mg-MOF-74 synthesized by adding different concentrations of NaAc.
Figure 1. XRD pattern of Mg-MOF-74 synthesized by adding different concentrations of NaAc.
Coatings 14 00383 g001
Figure 2. SEM images of Mg-MOF-74-N0 (a), Mg-MOF-74-N0.5 (b), Mg-MOF-74-N1 (c), and Mg-MOF-74-N2 (d).
Figure 2. SEM images of Mg-MOF-74-N0 (a), Mg-MOF-74-N0.5 (b), Mg-MOF-74-N1 (c), and Mg-MOF-74-N2 (d).
Coatings 14 00383 g002
Figure 3. N2 adsorption and desorption isotherms of Mg-MOF-74-N0 (a) and Mg-MOF-74-N2 (b).
Figure 3. N2 adsorption and desorption isotherms of Mg-MOF-74-N0 (a) and Mg-MOF-74-N2 (b).
Coatings 14 00383 g003
Figure 4. Thermogravimetric analysis of Mg-MOF-74 and Mg-MOF-74-N2.
Figure 4. Thermogravimetric analysis of Mg-MOF-74 and Mg-MOF-74-N2.
Coatings 14 00383 g004
Figure 5. CO2 dynamic adsorption penetration curves of Mg-MOF-74-N0 and Mg-MOF-74-N2 at 30 °C and 0.1 bar CO2 partial pressures.
Figure 5. CO2 dynamic adsorption penetration curves of Mg-MOF-74-N0 and Mg-MOF-74-N2 at 30 °C and 0.1 bar CO2 partial pressures.
Coatings 14 00383 g005
Figure 6. CO2 adsorption capacity of Mg-MOF-74-N2 after 10 absorption and desorption cycles at 30 °C and a 0.1 bar CO2 partial pressure.
Figure 6. CO2 adsorption capacity of Mg-MOF-74-N2 after 10 absorption and desorption cycles at 30 °C and a 0.1 bar CO2 partial pressure.
Coatings 14 00383 g006
Table 1. Pore volume, specific surface area, and pore size of Mg-MOF-74 and Mg-MOF-74-N2.
Table 1. Pore volume, specific surface area, and pore size of Mg-MOF-74 and Mg-MOF-74-N2.
SamplesSpecific Area (m2/g)Pore Volume (cm3/g)Pore Size (nm)
Mg-MOF-74570.30.2180.91
Mg-MOF-74-N2624.70.2640.92
Disclaimer/Publisher’s Note: The statements, opinions and data contained in all publications are solely those of the individual author(s) and contributor(s) and not of MDPI and/or the editor(s). MDPI and/or the editor(s) disclaim responsibility for any injury to people or property resulting from any ideas, methods, instructions or products referred to in the content.

Share and Cite

MDPI and ACS Style

Xin, C.; Hou, S.; Yu, L.; Zhou, X.; Fu, Y.; Yang, X.; Sun, W.; Yang, F.; Wang, X.; Liu, L. Controlled Synthesis of Mg-MOF-74 and Its CO2 Adsorption in Flue Gas. Coatings 2024, 14, 383. https://doi.org/10.3390/coatings14040383

AMA Style

Xin C, Hou S, Yu L, Zhou X, Fu Y, Yang X, Sun W, Yang F, Wang X, Liu L. Controlled Synthesis of Mg-MOF-74 and Its CO2 Adsorption in Flue Gas. Coatings. 2024; 14(4):383. https://doi.org/10.3390/coatings14040383

Chicago/Turabian Style

Xin, Chunling, Shufen Hou, Lei Yu, Xiaojing Zhou, Yunkai Fu, Xiaoteng Yang, Weiwei Sun, Fan Yang, Xia Wang, and Lili Liu. 2024. "Controlled Synthesis of Mg-MOF-74 and Its CO2 Adsorption in Flue Gas" Coatings 14, no. 4: 383. https://doi.org/10.3390/coatings14040383

Note that from the first issue of 2016, this journal uses article numbers instead of page numbers. See further details here.

Article Metrics

Back to TopTop