Next Article in Journal
Enhancement of the Electrochemical Performances of Composite Solid-State Electrolytes by Doping with Graphene
Next Article in Special Issue
A Novel Metal-Containing Mesoporous Silica Composite for the Decolorization of Rhodamine B: Effect of Metal Content on Structure and Performance
Previous Article in Journal
Development of Bio-Nanofluids Based on the Effect of Nanoparticles’ Chemical Nature and Novel Solanum torvum Extract for Chemical Enhanced Oil Recovery (CEOR) Processes
Previous Article in Special Issue
Tetracycline Removal by Hercynite-Biochar from the Co-Pyrolysis of Red Mud-Steel Slag-Sludge
 
 
Font Type:
Arial Georgia Verdana
Font Size:
Aa Aa Aa
Line Spacing:
Column Width:
Background:
Article

Thermal-Driven Formation of Silver Clusters Inside Na/Li FAUY Zeolites for Formaldehyde Detection

School of Materials Science and Engineering, Tongji University, Shanghai 201804, China
*
Author to whom correspondence should be addressed.
Nanomaterials 2022, 12(18), 3215; https://doi.org/10.3390/nano12183215
Submission received: 5 August 2022 / Revised: 1 September 2022 / Accepted: 13 September 2022 / Published: 16 September 2022
(This article belongs to the Special Issue Nanomaterials for Detection and Removal of Organic Pollutants)

Abstract

:
In this research, the LiY zeolite was firstly synthesized by using NaY as the parent zeolite; thereafter, the LiYAg and NaYAg zeolites created for formaldehyde gas detection were prepared with further Ag+-Li+/Na+ exchange and a mild thermal treatment at 300 °C to promote the formation of luminescent Ag CLs. The spectra experimental results indicated that Ag CLs showed stronger and blue-shifted emissions in LiYAg compared with in NaYAg, and the emission intensity of Ag CLs in both zeolites monotonously decreased when exposed to increasing formaldehyde gas content. Moreover, the linear dependence of the Ag CLs’ emission intensity variation on formaldehyde content indicated a reliable method for fast and sensitive formaldehyde detection. According to the XPS, UV–vis absorption, and N2 adsorption–desorption isotherm studies, the formaldehyde-gas-induced luminescence quenching of Ag CLs is due to the formation of Ag2O and Ag NPs, in which the higher content of Ag+/Ag0 redox couples in LiYAg and larger surface area of NaYAg benefit the precise detection of formaldehyde gas in low- and high-content ranges, respectively. Furthermore, the blue-shifted peak position and widened FWHM of Ag CLs can also be used for the indication of formaldehyde gas and the detection limit of NaYAg and LiYAg, which both meet with the standards of the WHO and OSHA.

1. Introduction

Noble metal clusters consisting of only a few atoms or ions exhibit outstanding catalytic and optical properties due to their molecule-like structures and energetics, which are quite different from their nanoparticle and bulk metal counterparts [1,2,3]. Recent studies suggest that the silver clusters (Ag CLs) possess intriguing luminescence properties, with emissions covering the visible range and external quantum efficiency up to 97%, which is mainly governed by the clusters’ sizes, charges, and geometries [4,5,6]. However, precise control of Ag CLs’ luminescence properties remains challenging due to their tendency to aggregate into larger particles to reduce surface energy, thus irreversibly losing their emissive abilities [7,8,9]. Various host materials and synthesis approaches have been applied so far to stabilize Ag CLs of various sizes and chemical states, such as using DNA, polymers, rigid glasses, and zeolites [8,10,11].
Zeolites are porous materials with molecular-sized channels and cages that act as promising scaffolds for luminescent Ag CLs to avoid aggregating through spatial restrictions [3,9,12]. Benefitting from the diverse framework topologies, high cation exchange rates, tunable Si/Al ratios, and high thermal stabilities, the Ag+ can be readily loaded into zeolites and the luminescence properties of Ag CLs formed through subsequent external driven energy can be flexibly manipulated for diverse applications, such as white LEDs, imaging, and sensors [6,7,13,14]. It was reported that the emission peak wavelengths of Ag CLs in FAU zeolites are Si/Al ratio, extra framework cation, and thermal treatment condition dependent, and can be turned from 460 to 560 nm [7,15,16,17]. Further comparisons of the luminescence properties of Ag CLs formed with X-ray irradiation and thermal treatment indicate that the latter promotes the formation of luminescent clusters with specific small nuclearities, while the former produces a wide distribution of cluster species and larger nanoparticles [18,19]. Therefore, thermal treatment has been commonly used to promote the even formation of Ag CLs, and recent studies demonstrated that thermal treatment temperature influences the water content and stability of Ag CLs in LAT and FAU zeolites [6,20]. Furthermore, the thermal treatment atmosphere also manipulates the formation of Ag CLs in FAUX zeolites, the smaller Ag CLs (Ag22+, Ag3+, and Ag32+) can be formed under the oxygen flow, while the larger Ag CLs (Ag4n+ and Ag8m+) can be formed under a hydrogen atmosphere [21,22]. Additionally, extra framework modifications through Li+-Na+ exchange before Ag+ loading have proved to be ideal for improving the stability and luminescence intensity of Ag CLs because of the small radius and high affinity of Li+ to coordinate with zeolite framework oxygen [6,16,17].
The volatile organic solvent formaldehyde (HCHO) is a major indoor pollutant released from buildings and decorative materials that is detrimental to human health and may cause serious organ damage and even central nervous system injury [23,24,25]. The World Health Organization (WHO) and Occupational Safety and Health Administration (OSHA) have established that the long-term exposure-level limits for formaldehyde are 0.08 and 0.75 ppm, respectively [20,26]. Current formaldehyde detection methods include liquid/gas chromatography, spectroscopy, colorimetry, and electrochemical sensing; however, the practical application of these methods remains a big challenge because they are either highly cost- or time-consuming, involved in harmful reagents, or hard to achieve with high efficiency and sensitivity [20,27,28,29]. Fast-response, high-accuracy, and low-content formaldehyde-detection approaches are still under development.
In this study, faujasite zeolite with a high ion-exchange rate was used as a scaffold for Ag NCs to achieve a bright emission under UV excitation. The LiY zeolite was firstly synthesized by using NaY as the parent zeolite; thereafter, the LiYAg and NaYAg zeolites used for formaldehyde gas detection were prepared with a further Ag+-Li+/Na+ exchange and mild thermal treatment at 300 °C to promote the formation of luminescent Ag CLs. Under UV excitation, the Ag CLs showed stronger and blue-shifted emissions in LiYAg compared with in NaYAg, and the emission intensities of Ag CLs in both zeolites decreased when exposed to formaldehyde gas. The XPS, UV–vis absorption, and N2 adsorption–desorption isotherm results indicated that the formaldehyde-gas-induced luminescence quenching is due to the formation of Ag2O and Ag NP. The linear fitting between the formaldehyde concentration and the emission intensity variations of Ag CLs indicated LiYAg and NaYAg can be used for the precise detection of formaldehyde in a wide range.

2. Materials and Methods

2.1. Materials and Reagents

We purchased commercially available zeolite Na-FAUY ((Na6.5+)[Al6.5Si17.5O48], denoted as NaY) with SiO2/Al2O3 = 5.1 in powder form from Alfa Aesar. We obtained LiNO3 (99.99%, metals basis) from Aladdin Chemical Co., Ltd., Shanghai, China. We purchased AgNO3 (99.8%) from Sinopharm Chemical Reagent Co., Ltd., Shanghai, China. We obtained formaldehyde (HCHO, 37–40 wt% in water, AR) from Tansoole, Shanghai, China. We used all the materials and reagents as received without any further purification and dissolved all the aqueous solutions in deionized water.

2.2. Preparation of LiY Zeolite

The LiY zeolites were obtain from Li+-exchange on parent NaY zeolites. Each 1 g NaY zeolite was suspended in a highly concentrated 50 mL LiNO3 aqueous solution (5 mol/L). The suspension was agitated for 24 h at 80 °C, and then recovered by centrifugation, washed with deionized water several times and dried overnight at 80 °C.

2.3. Preparation of Ag CLs-Loaded NaY and LiY Zeolites

We obtained Ag CLs-loaded NaY and LiY zeolites by Ag+ exchange on NaY and LiY zeolites and a subsequent calcination procedure. Firstly, we suspended each 1 g NaY and LiY zeolite in 50 mL AgNO3 aqueous solution (30 mmol/L) and then agitated for 1.5 h at 40 °C in dark. Subsequently, we recovered the suspension by centrifugation, washed with deionized water several times, and dried overnight at 80 °C. Finally, we calcined the resultant Ag+-exchanged NaY and LiY zeolites at 300 °C for 2 h in air and sealed in dried containers in dark for further analysis. We denoted the final products as NaYAg and LiYAg, respectively.

2.4. Formaldehyde Detection

The climate chamber for formaldehyde detection is self-made and is shown Figure S1. Firstly, we diluted 0.3 mL formaldehyde aqueous solution to 2000, 1000, 250, and 100 mL, corresponding to the actual concentrations of 0.05, 0.10, 0.40, and 1.00 mg/1000 L, respectively. We dropped each concentration of 10 μL formaldehyde aqueous solution into glass-surface vessel and then put it into the polytetrafluoroethylene (PTFE) container; meanwhile, we placed 0.5 g LiYAg and 0.5 g NaYAg powders in two separated crucibles and covered before putting into the same PTFE container. After evaporating for 2 h at 25 °C, the formaldehyde concentration in the PTFE container reaches a plateau, and then we removed the cover to expose LiYAg and NaYAg powders to formaldehyde gas for 30 min. We monitored the formaldehyde concentrations in the container by commercial test strip at the same time. We denoted the samples explored in formaldehyde gases as M-x, M = LiYAg, or NaYAg, x = 0.05, 0.10, 0.40, and 1.00 mg/1000L, respectively, according to the formaldehyde aqueous solution concentration. We denoted the LiYAg and NaYAg exposed to formaldehyde aqueous solution without dilution as LiYAg-Excess and NaYAg-Excess, respectively. For consistency, we also exposed the NaYAg and LiYAg in non-formaldehyde atmosphere for 30 min in the PTFE container and labeled them as LiYAg-Original and NaYAg-Original, respectively.

2.5. Measurements

We carried out the Raman spectra on HR Evolution, Longjumeau, France, scanned in the range of 200–900 cm−1. We recorded the X-ray diffraction (XRD) patterns on Rigaku Smartlab9 diffractometer, Tokyo, Japan, with Cu-Kα radiation (λ = 1.5406 Å). We measured the photoluminescence (PL) and the photoluminescence of excitation (PLE) spectra with Edinburgh FLS980, Edinburgh, UK. We carried out the X-ray photoelectron spectroscopy (XPS) measurements on Thermo ESCALAB 250XI Waltham, MA, USA, by using Al ( = 1486.6 eV, 650 μm of beam spot) as the incident radiation source, and we used the electron flood gun to minimize surface charging effect. We detected the high-resolution XPS spectra of Ag 3d with 30 eV pass energy and the Ag Auger spectra with 40 eV pass energy. We measured the UV–vis absorbance spectra in the wavelength range of 200–700 nm on Shimadzu UV-3600i Plus spectrophotometer, Kyoto, Japan, at room temperature and applied attenuators to remove the effects of background and noise. We measured N2 adsorption–desorption isotherm by Micromeritics ASAP2020, Atlanta, GA, USA, at 77 K and calculated the total surface area by Brunauer–Emmett–Teller (BET) method.

3. Results and Discussion

3.1. Structural and Chemical Analysis

Charge-balancing cations coordinated to the zeolite framework ions can modify framework vibrations through electrostatic interaction. Figure 1 shows the Raman spectra of LiY and NaY have two main bands located at 360 and 506 cm−1, which can be attributed to the bending vibration of the six- (δ 6MR) and four-membered ring (δ 4MR), respectively. The high frenquency shift of the δ 4MR for LiY is caused by the increased T-O-T bonding force and reduced T-O-T angle brought by the substitution of Li+ for Na+ [30,31]. To study the effects of ion exchange on the phase purity and structure of the parent zeolite, the XRD patterns of LiY, NaYAg, and LiYAg are compared with that of NaY in Figure 2b. LiY, NaYAg, and LiYAg all maintain the structure of the parent NaY, while NaYAg and LiYAg show decreased diffraction intensities due to the later thermal treatment [8,32]. It is noticed that the diffraction peak intensities of the parent NaY zeolite (I) follow I331 > I220 > I311, which changed to I331 > I311 > I220 for LiY, NaYAg, and LiYAg. As the peaks of the (331), (311), and (220) facets are colsely related to the locations of cations in zeolites, this relative diffraction peak intensity varition can be attributed to the redistribution of the intra-zeolite charge-balancing cations of Na+, Li+, and Ag+ [33,34]. Furthermore, the increased diffraction intensity of the (622) facet in NaYAg and LiYAg also indicates the succssful incorporation of Ag+ [8,17].
The XPS survey spectra of NaY, LiY, NaYAg, and LiYAg are shown in Figure 1c, from which the Al 2p, Si 2p, C 1s, O 1s, and Na 1s peaks can be observed for all the samples, and the Li 1s and Ag 3d peaks can be observed in LiY, LiYAg, and NaYAg. The XPS chemical composition in Figure 1d shows that Na content drastically decreased from 10.29 atomic% in NaY to 3.12 atomic% in LiY due to the successful introduction of 6.32 atomic% Li. It is noticed that after Ag+ exchanged under the same conditions, the Ag content in NaYAg and LiYAg had different values of 4.41 and 4.63 atomic%, respectively. The different Ag content in NaYAg and LiYAg indicates the exchange efficiency of Ag+ is influenced by extra-framework cations, and the Li+-Ag+ has a higher exchange rate than Na+-Ag+, which has also been reported in previous studies [16,17].

3.2. Luminescence Property and Chemical State of Ag CLs

It is generally agreed that the stable Ag3n+ clusters can be formed inside the D6r cages of Ag+-exchanged FAUY zeolites after high-temperature thermal treatment at around 600 °C, which gives off bright emissions under UV excitation [18,35,36]. In this study, a low temperature of 300 °C was carried out to promote the formation of luminescent Ag CLs in the Ag+-exchanged NaY and LiY zeolites. The PLE and PL spectra of LiYAg and NaYAg in Figure 2 both show a strong excitation band peaked at 306 nm together with a very weak shoulder located at 265 nm, and a very broad emission band in the range of 450–600 nm, indicating the formation of Ag3n+ clusters [4,7,8]. Previous studies indicated that the Ag CLs formed under mild thermal treatment tended to be located outside the cavities and cages of FAUY zeolite, making them less stable with the surrounding atmosphere [20]. It is noticed that the emission intensity of Ag CLs is stronger in LiYAg than in NaYAg. This is because Ag content is higher in LiYAg than in NaYAg and, more importantly, Li+ can make Ag+ move to appropriate sites easily to form Ag CLs owing to its smaller radius than Na+, which promotes the formation and stabilization of Ag CLs due to their high affinity to coordinate with framework oxygen [6,16,17]. Moreover, the emission peak wavelength of Ag CLs slightly blue-shifted from 526 nm in NaYAg to 522 nm in LiYAg, which can be attributed to the reduced lattice parameter after the replacement of Na+ by Li+ [17,30].
Furthermore, the XPS measurement was carried out to identify the chemical state of silver species in LiYAg and NaYAg. The high-resolution XPS spectra of Ag 3d in Figure 3a presents two photoelectron peaks attributed to Ag 3d5/2 and Ag 3d3/2. Because of the small chemical shift and the binding energy overlap of Ag 3d in different silver species [1,37], the high-resolution XPS spectra of Ag 3d show no difference for LiYAg and NaYAg. Figure 3b shows Ag M4N45N45 Auger spectra, in which the two bands with discriminable kinetic energies for LiYAg and NaYAg can be attributed to Ag M4N45N45 and Ag M5N45N45, respectively (see Table S1). Therefore, the Auger parameter of Ag 3d, which is more sensitive to the chemical bonding environment, was calculated through the sum of the binding energy of Ag 3d5/2 and the kinetic energy of Ag M4N45N45 (Auger parameter = Ag 3d5/2 + Ag M4N45N45) [19,36,37], which are 722.3 and 722.5 eV for LiYAg and NaYAg, respectively. The small chemical shift compared with Ag2O (724.1 eV) and the large chemical shift compared with Ag NPs (726.0 eV) and metallic silver indicate the formation of Ag CLs in both zeolites, while the higher Auger parameter of Ag MNN in NaYAg than in LiYAg can be ascribed to the different extra-frame cations in the host zeolite [17,19,36,37].

3.3. Formaldehyde Sensor and Luminescence Quenching Mechanism

Figure 4a,b show the PL spectra of Ag CLs in LiYAg and NaYAg after exposing to different contents of formaldehyde gases. It can be seen that the emission intensity of Ag CLs in LiYAg and NaYAg both monotonously decrease with increasing-content formaldehyde gas, and the luminescence quenching on the whole is much more evident for NaYAg, which is in accordance with the results of previous research that the Ag CLs were more stable in Li-zeolite than in Na-zeolite [6,16,38]. It is worth mentioning that once exposed to formaldehyde gases, even a low concentration of 0.05 mg/m3 (lower than the limited permissible concentrations of WHO and OSHA), the Ag CLs show blue-shifted emissions and increased full width at half-maximum (FWHM) in both LiYAg and NaYAg, indicating the sensitive detection of very-low-content formaldehyde. The digital photos of NaYAg and LiYAg zeolite powders before and after being exposed to various contents of formaldehyde gases under natural light are shown in Figure 4c. The colors of the LiYAg and NaYAg powders both become dark with increasing-content formaldehyde gas, which is in line with the PL results.
According to the PL spectra in Figure 4a, the relationships between formaldehyde concentration (x) and the emission intensity variation (y = Ix/Ioriginal) of Ag CLs in LiYAg and NaYAg were plotted in Figure 4d, which can be linearly fitted with Equations (1) and (2).
y = A 1 × e x t 0 + A 2
where A1 = 0.30, A2 = 0.69, t0 = 0.25, R2 = 0.991.
y = B 2 B 1 1 + x x 0 p + B 2
where B1 = 1.00, B2 = 0.51, x0 = 0.25, p = 2.43, R2 = 0.998;
The first derivative is bigger for the fitting curve from Equation (1) than the curve from Equation (2) when x < 0.18 mg/m3, indicating that LiYAg can more sensitively detect low-content formaldehyde than NaYAg. This can be ascribed to the higher Ag atomic content (See Figure 1d) or the increased quantity of Ag+/Ag0 redox couples that constitute Ag CLs in LiYAg. It is generally agreed that the Ag+/Ag0 redox couples can generate oxygen vacancies (   V 0 ¨ ) through Equation (3), and the   V 0 ¨ can effectively promote the absorption of formaldehyde gas [8,26,39,40].
4 Ag + + 2 O 2 4 Ag 0 + O 2 +   V 0 ¨
Interestingly, after exposing to high concentrations of formaldehyde gases, Ix/Ioriginal shows a more significant decrease in NaYAg than in LiYAg. In order to figure out the reason for the different spectra responses to high-content formaldehyde gas, the N2 adsorption–desorption isotherms of LiYAg and NaYAg were measured (See Figure S2), and we found both exhibited typical type I adsorption isotherm of microporous phase [41,42,43]. Application of the BET model confirms the surface area of LiYAg and NaYAg are 713.8 and 764.3 m2/g, respectively, indicating a higher adsorption capability of NaYAg than LiYAg. Therefore, NaYAg can adsorb more formaldehyde gases than LiYAg when exposed to high-content formaldehyde gases, resulting in more significantly decreased emission intensity. Therefore, the higher content of Ag+/Ag0 redox couples in LiYAg and larger surface area of NaYAg can benefit the precise detection of formaldehyde gas in low- and high-content ranges, respectively.
To further investigate the mechanism that is responsible for the formaldehyde-gas-induced luminescence quenching of Ag CLs, the UV–vis absorbance spectra were firstly measured for LiYAg and NaYAg before and after exposing to 0.40 mg/m3 and excess formaldehyde gases. As shown Figure 5, the strong absorption band peaked at 213 nm, which can be ascribed to the 4d10→4d95s1 electronic transition of isolated silver ions in FAU and LTA zeolites, and the absorptions located at 275 and 324 nm belonged to the Ag3n+ clusters confined in FAU zeolites [6,17,18]. It is noticed that the absorption intensity of Ag+ is very close for LiYAg and NaYAg, while that of Ag CLs is stronger in LiYAg than in NaYAg, indicating more Ag CLs were formed in LiYAg. After exposing to formaldehyde gas, the absorption intensity of Ag CLs rapidly decreased for both LiYAg-0.40 and NaYAg-0.40, and further reduced in LiYAg-Excess and NaYAg-Excess. This is in accordance with the PL spectra in Figure 4a,b. Moreover, the surface plasma resonance (SPR) absorption band located around 450 nm can be observed for NaYAg-Excess and LiYAg-Excess, indicating the formation of Ag NPs [7,8,17]. Therefore, we speculate that the exposure to formaldehyde gas reduced the luminescence center number through inducing the transformation from ionic Ag CLs to metallic Ag NPs, thus resulting in quenched emission intensities.
Based on the above considerations, it is necessary to identify the chemical state of silver before and after exposing to formaldehyde gas. According to the XPS data in Table S2, we calculated the Auger parameter of Ag in LiYAg and NaYAg before and after exposing to 0.05 and 0.40 mg/1000L, as well as excess formaldehyde gases. As shown in Figure 6, the Auger parameter of Ag in LiYAg-x and NaYAg-x firstly increases and then decreases after exposure to high-content formaldehyde, and the increase and decrease in Auger parameter indicate the reduction and oxidation of Ag CLs, respectively [32,37,44]. On the one hand, the Ag+ that constitutes Ag CLs can acquire electrons from framework oxygen, hydration water, and formaldehyde to form Ag0 and   V 0 ¨ through the above Equation (3) [8,15,45,46]. On the other hand, the Ag0 in Ag CLs can be oxidized to Ag2O through Equation (4) [20,47].
4 Ag 0 + O 2 2 Ag 2
Therefore, the Ag+/Ag0 redox couples can reach an eqiuilibrium through the reactions described in Equations (3) and (4) when exposed to formaldehyde gases. Under a low-content formaldehyde atmosphere, the oxidation of Ag0 into Ag+ through Equation (4) dominates, resulting in decreased Auger parameter; however, in high-content formaldehyde atmospheres, there are excessive formations of Ag0 through Equation (3) because Ag+ can acquire more electrons from O2− in the adsorbed formaldehyde, leading to an increased Auger parameter. The excessively formed Ag0 can aggregate into large Ag NPs, which allows the further increase of the Auger parameter in accordance with the absorption in Figure 5. Consequently, the formaldehyde-gas-induced luminescence quenching of Ag CLs is due to the dynamic formation of Ag2O and Ag NPs, and the adsorbed formaldehyde can be oxidized into water molecules and carbon dioxide, as described in Equations (5) and (6) [20,26,48].
1 2 O 2   gas +   e     O ads
HCHO + 2 O ads     CO 2 +   H 2 O   +   e

4. Conclusions

In conclusion, the LiY zeolite was firstly synthesized by using NaY as the mother zeolite; thereafter, the Ag CLs loaded LiYAg and NaYAg zeolites with mild thermal treatment were prepared. The spectra results indicated that Ag CLs show stronger and blue-shifted emissions in LiYAg compared with in NaYAg. The emission intensity of Ag CLs monotonously decreases when exposed to increasing contents of formaldehyde gas in both zeolites, and the linear fittings between the formaldehyde concentration and the emission intensity variations of Ag CLs were obtained for LiYAg and NaYAg. The XPS, UV–vis absorption, and N2 adsorption–desorption isotherm results indicated that the formaldehyde-gas-induced luminescence quenching of Ag CLs is due to the dynamic formation of Ag2O and Ag NPs, and the higher content of Ag+/Ag0 redox couples in LiYAg and the larger surface area of NaYAg benefit the precise detection of formaldehyde gas in low- and high-content ranges, respectively. Furthermore, the blue-shift peak position and widened Ag CLs FWHM can also be used for the indication of formaldehyde gas and the low detection limit of 0.05 mg/1000 L for NaYAg and LiYAg, which meet the WHO and OSHA standards.

Supplementary Materials

The following supporting information can be downloaded at: https://www.mdpi.com/article/10.3390/nano12183215/s1, Figure S1: Schematic diagram of experimental installation for the detection of formaldehyde gas; Figure S2: N2 adsorption–desorption isotherms of NaYAg and LiYAg and the corresponding BET surface area; Table S1: Binding energies and Auger parameters of Ag in NaYAg and LiYAg; Table S2: Binding energies and Auger Parameters of Ag MNN in NaYAg and LiYAg before and after exposing to air and different contents of formaldehyde atmosphere.

Author Contributions

Sample preparation, spectra and XPS measurements, original draft preparation, J.Y.; writing—review and editing, supervision, funding acquisition, project administration, S.Y.; XPS measurement and data analysis, X.X.; XRD measurement and data analysis, L.P.; spectra measurement and data analysis, P.L.; spectra measurement, H.L.; review and funding acquisition, D.W. All authors have read and agreed to the published version of the manuscript.

Funding

This work was financially supported by the National Natural Science Foundation of China (Nos.51872200, 51772210), the Natural Science Foundation of Shanghai (No.18ZR1441900), and the National Key Research and Development Projects (No.2018YFC1106302).

Institutional Review Board Statement

Not applicable.

Informed Consent Statement

Not applicable.

Data Availability Statement

Not applicable.

Conflicts of Interest

The authors declare no conflict of interest.

References

  1. Grandjean, D.; Coutiño-Gonzalez, E.; Cuong, N.T.; Fron, E.; Baekelant, W.; Aghakhani, S.; Schlexer, P.; D’Acapito, F.; Banerjee, D.; Roeffaers, M.B.J.; et al. Origin of the bright photoluminescence of few-atom silver clusters confined in LTA zeolites. Science 2018, 361, 686–690. [Google Scholar] [CrossRef] [PubMed]
  2. Chai, Y.; Shang, W.; Li, W.; Wu, G.; Dai, W.; Guan, N.; Li, L. Noble Metal Particles Confined in Zeolites: Synthesis, Characterization, and Applications. Adv. Sci. 2019, 6, 1900299. [Google Scholar] [CrossRef] [PubMed]
  3. Romolini, G.; Steele, J.A.; Hofkens, J.; Roeffaers, M.B.J.; Coutino-Gonzalez, E. Tunable Luminescence from Stable Silver Nanoclusters Confined in Microporous Zeolites. Adv. Opt. Mater. 2021, 9, 2100526. [Google Scholar] [CrossRef]
  4. Coutino-Gonzalez, E.; Roeffaers, M.B.J.; Dieu, B.; De Cremer, G.; Leyre, S.; Hanselaer, P.; Fyen, W.; Sels, B.; Hofkens, J. Determination and Optimization of the Luminescence External Quantum Efficiency of Silver-Clusters Zeolite Composites. J. Phys. Chem. C 2013, 117, 6998–7004. [Google Scholar] [CrossRef]
  5. Kikukawa, Y.; Kuroda, Y.; Suzuki, K.; Hibino, M.; Yamaguchi, K.; Mizuno, N. A discrete octahedrally shaped [Ag6]4+ cluster encapsulated within silicotungstate ligands. Chem. Commun. 2013, 49, 376–378. [Google Scholar] [CrossRef]
  6. Coutino-Gonzalez, E.; Baekelant, W.; Grandjean, D.; Roeffaers, M.B.J.; Fron, E.; Aghakhani, M.S.; Bovet, N.; Auweraer, M.V.D.; Lievens, P.; Vosch, T.; et al. Thermally activated LTA(Li)-Ag zeolites with water-responsive photoluminescence properties. J. Mater. Chem. C 2015, 3, 11857–11867. [Google Scholar] [CrossRef]
  7. Yao, D.; Xu, S.; Wang, Y.; Li, H. White-emitting phosphors with high color-rendering index based on silver cluster-loaded zeolites and their application to near-UV LED-based white LEDs. Mater. Chem. Front. 2019, 3, 1080–1084. [Google Scholar] [CrossRef]
  8. Yu, J.; Ye, S.; Shi, Y.; Liao, H.; Xv, X.; Wang, D. Confinement of Highly Luminescent Silver Nanoclusters in FAUY Zeolite: A Study on the Formation Effects of Silver Nanoclusters and the Sensitization of Tb3+. ACS Appl. Nano Mater. 2021, 4, 6290–6298. [Google Scholar] [CrossRef]
  9. Coutino-Gonzalez, E.; Baekelant, W.; Steele, J.A.; Kim, C.W.; Roeffaers, M.B.J.; Hofkens, J. Silver Clusters in Zeolites: From Self-Assembly to Ground-Breaking Luminescent Properties. Acc. Chem. Res. 2017, 50, 2353–2361. [Google Scholar] [CrossRef]
  10. Wen, Q.L.; Peng, J.; Liu, A.Y.; Hu, Y.L.; Wang, J.; Ling, J.; Cao, Q.E. Fluorescent silver nanoclusters stabilized in guanine-enhanced DNA hybridization for recognizing different small biological molecules. J. Lumin. 2020, 221, 117038. [Google Scholar] [CrossRef]
  11. Kuznetsov, A.S.; Tikhomirov, V.K.; Shestakov, M.V.; Moshchalkov, V.V. Ag nanocluster functionalized glasses for efficient photonic conversion in light sources, solar cells and flexible screen monitors. Nanoscale 2013, 5, 10065–10075. [Google Scholar] [CrossRef]
  12. Imakita, K.; Lin, H.; Fujii, M. Ag and Dy doped zeolite as a broadband phosphor. Opt. Mater. 2014, 38, 75–79. [Google Scholar]
  13. Cametti, G.; Scheinost, A.C.; Giordani, M.; Churakov, S.V. Framework Modifications and Dehydration Path of a Ag+-Modified Zeolite with STI Framework Type. J. Phys. Chem. C 2019, 123, 13651–13663. [Google Scholar] [CrossRef]
  14. De Cremer, G.; Sels, B.F.; Hotta, J.; Roeffaers, M.B.; Bartholomeeusen, E.; Coutino-Gonzalez, E.; Valtchev, V.; Vos, D.E.D.; Vosch, T.; Hofkens, J. Optical encoding of silver zeolite microcarriers. Adv. Mater. 2010, 22, 957–960. [Google Scholar] [CrossRef]
  15. Cremer, G.D.; Coutiño-Gonzalez, E.; Roeffaers, M.B.J.; Moens, B.; Ollevier, J.; Auweraer, M.V.d.; Schoonheydt, R.; Jacobs, P.A.; Schryver, F.C.D.; Hofkens, J.; et al. Characterization of Fluorescence in Heat-Treated Silver-Exchanged Zeolites. J. Am. Chem. Soc. 2009, 131, 3049–3056. [Google Scholar] [CrossRef]
  16. Johan, E.; Kanda, Y.; Matsue, N.; Itagaki, Y.; Aono, H. Whitish fluorescence of partially Ag-exchanged zeolite Y affected by coexisting cations. J. Lumin. 2019, 213, 482–488. [Google Scholar] [CrossRef]
  17. Yu, J.; Ye, S.; Liao, H.; Xv, X.; Wang, D. Luminescence Control of Silver Nanoclusters by Tailoring Extra-Framework Cations in FAU-Y Zeolite: Implications for Tunable Emission. ACS Appl. Nano Mater. 2021, 4, 13692–13699. [Google Scholar] [CrossRef]
  18. Coutino-Gonzalez, E.; Grandjean, D.; Roeffaers, M.; Kvashnina, K.; Fron, E.; Dieu, B.; Cremer, G.D.; Lievens, P.; Sels, B.; Hofkens, J. X-ray irradiation-induced formation of luminescent silver clusters in nanoporous matrices. Chem. Commun. 2014, 50, 1350–1352. [Google Scholar] [CrossRef]
  19. Fenwick, O.; Coutino-Gonzalez, E.; Richard, F.; Bonacchi, S.; Baekelant, W.; de Vos, D.; Roeffaers, M.B.J.; Hofkens, J.; Samori, P. X-ray-Induced Growth Dynamics of Luminescent Silver Clusters in Zeolites. Small 2020, 16, 2002063. [Google Scholar] [CrossRef]
  20. Yao, D.; Wang, Y.; Li, H. Silver clusters based sensor for Low content formaldehyde detection in colorimetric and fluorometric dual Mode. Sens. Actuators B Chem. 2020, 305, 127451. [Google Scholar] [CrossRef]
  21. Lee, S.H.; Kim, Y.; Seff, K. Weak Ag+-Ag+ bonding in zeolite X. Crystal structures of Ag92Si100Al92O384 hydrated and fully dehydrated in flowing oxygen. Microporous Mesoporous Mater. 2000, 41, 49–59. [Google Scholar] [CrossRef]
  22. Kim, S.Y.; Kim, Y.; Seff, K. Two Crystal Structures of Fully Dehydrated, Fully Ag+-Exchanged Zeolite X. Dehydration in Oxygen Prevents Ag+ Reduction. Without Oxygen, Ag8n+ (Td) and cyclo-Ag4m+ (near S4) Form. J. Phys. Chem. B 2003, 107, 6938–6945. [Google Scholar] [CrossRef]
  23. Wang, Y.; Dai, C.; Chen, B.; Wang, Y.; Shi, C.; Guo, X. Nanoscale HZSM-5 supported PtAg bimetallic catalysts for simultaneous removal of formaldehyde and benzene. Catal. Today 2015, 258, 616–626. [Google Scholar] [CrossRef]
  24. Zhang, L.; Xie, Y.; Jiang, Y.; Li, Y.; Wang, C.; Han, S.; Luan, H.; Meng, X.; Xiao, F.S. Mn-promoted Ag supported on pure siliceous Beta zeolite (Ag/Beta-Si) for catalytic combustion of formaldehyde. Appl. Catal. B Environ. 2020, 268, 118461. [Google Scholar] [CrossRef]
  25. Wang, W.; Zhang, D.; Sun, P.; Ji, Z.; Duan, J. High efficiency photocatalytic degradation of indoor formaldehyde by Ag/g-C3N4/TiO2 composite catalyst with ZSM-5 as the carrier. Microporous Mesoporous Mater. 2012, 322, 111134. [Google Scholar] [CrossRef]
  26. Sun, Y.; Wang, J.; Du, H.; Li, X.; Wang, C.; Hou, T. Formaldehyde gas sensors based on SnO2/ZSM-5 zeolite composite nanofibers. J. Alloys Compd. 2021, 868, 159140. [Google Scholar] [CrossRef]
  27. Zhang, K.; Liu, C.; Li, S.; Fan, J. A hydrophobic deep eutectic solvent based vortex-assisted liquid-liquid microextraction for the determination of formaldehyde from biological and indoor air samples by high performance liquid chromatography. J. Chromatogr. A 2019, 1589, 39–46. [Google Scholar] [CrossRef]
  28. Khosropour, H.; Rezaei, B.; Alinajafi, H.A.; Ensafi, A.A. Electrochemical sensor based on glassy carbon electrode modified by polymelamine formaldehyde/graphene oxide nanocomposite for ultrasensitive detection of oxycodone. Mikrochim. Acta 2021, 188, 1. [Google Scholar] [CrossRef]
  29. Fang, Y.; Ren, G.; Li, M.; Yang, Y.; Guo, D.Y.; Pan, Q. Sensitively liquid and gaseous detection of formaldehyde based on a supramolecular organic framework. Sens. Actuators B Chem. 2021, 349, 130726. [Google Scholar] [CrossRef]
  30. Baekelant, W.; Aghakhani, S.; Coutino-Gonzalez, E.; Kennes, K.; D’Acapito, F.; Grandjean, D.; Auweraer, M.V.d.; Lievens, P.; Roeffaers, M.B.J.; Hofkens, J.; et al. Shaping the Optical Properties of Silver Clusters Inside Zeolite A via Guest-Host-Guest Interactions. J. Phys. Chem. Lett. 2018, 9, 5344–5350. [Google Scholar] [CrossRef]
  31. Price, L.; Leung, K.; Sartbaeva, A. Local and Average Structural Changes in Zeolite A upon Ion Exchange. Magnetochemistry 2017, 3, 42. [Google Scholar] [CrossRef] [Green Version]
  32. Yu, J.; Ye, S.; Shi, Y.; Liao, H.; Wang, D. Thermally formation and luminescent performance of silver nanoclusters confined within LTA zeolites. J. Alloys Compd. 2021, 857, 157614. [Google Scholar] [CrossRef]
  33. Salavati-Niasari, M. Synthesis and characterization of 18- and 20-membered hexaaza macrocycles containing pyridine manganese(II) complex nanoparticles dispersed within nanoreactors of zeolite-Y. Polyhedron 2009, 28, 2321–2328. [Google Scholar] [CrossRef]
  34. Ferreira, L.; Fonseca, A.M.; Botelho, G.; Aguiar, C.A.; Neves, I.C. Antimicrobial activity of faujasite zeolites doped with silver. Microporous Mesoporous Mater. 2012, 160, 126–132. [Google Scholar] [CrossRef]
  35. Altantzis, T.; Coutino-Gonzalez, E.; Baekelant, W.; Martinez, G.T.; Abakumov, A.M.; Tendeloo, G.V.; Roeffaers, M.B.J.; Bals, S.; Hofkens, J. Direct Observation of Luminescent Silver Clusters Confined in Faujasite Zeolites. ACS Nano 2016, 10, 7604–7611. [Google Scholar] [CrossRef]
  36. Fenwick, O.; Coutino-Gonzalez, E.; Grandjean, D.; Baekelant, W.; Richard, F.; Bonacchi, S.; Vos, D.D.; Lievens, P.; Roeffaers, M.; Hofkens, J.; et al. Tuning the energetics and tailoring the optical properties of silver clusters confined in zeolites. Nat. Mater. 2016, 15, 1017–1022. [Google Scholar] [CrossRef]
  37. Fonseca, A.M.; Neves, I.C. Study of silver species stabilized in different microporous zeolites. Microporous Mesoporous Mater. 2013, 181, 83–87. [Google Scholar] [CrossRef]
  38. Aono, H.; Yahara, K.; Johan, E.; Itagaki, Y. Effect of coexisting lithium content on fluorescent properties of silver ion-exchanged LTA zeolite. J. Ceram. Soc. Jpn. 2020, 128, 670–676. [Google Scholar] [CrossRef]
  39. Liu, J.; Zhang, L.; Cheng, B.; Fan, J.; Yu, J. A high-response formaldehyde sensor based on fibrous Ag-ZnO/In2O3 with multi-level heterojunctions. J. Hazard. Mater. 2021, 413, 125352. [Google Scholar] [CrossRef]
  40. Li, N.; Fan, Y.; Shi, Y.; Xiang, Q.; Wang, X.; Xu, J. A low temperature formaldehyde gas sensor based on hierarchical SnO/SnO2 nano-flowers assembled from ultrathin nanosheets: Synthesis, sensing performance and mechanism. Sens. Actuators B Chem. 2019, 294, 106–115. [Google Scholar] [CrossRef]
  41. Pala-Rosas, I.; Contreras, J.L.; Salmones, J.; Zeifert, B.; López-Medina, R.; Navarrete-Bolaños, J.; Hernández-Ramírez, S.; Pérez-Cabrera, J.; Fragoso-Montes de Oca, A. A Catalytic Deactivation of HY Zeolites in the Dehydration of Glycerol to Acrolein. Catalysts 2021, 11, 360. [Google Scholar] [CrossRef]
  42. Batistela, V.R.; Fogaça, L.Z.; Fávaro, S.L.; Caetano, W.; Fernandes-Machado, N.R.C.; Hioka, N. ZnO supported on zeolites: Photocatalyst design, microporosity and properties. Colloids Surf. A 2017, 513, 20–27. [Google Scholar] [CrossRef]
  43. Wang, J.; Li, M.; Fu, Y.; Amoo, C.C.; Jiang, Y.; Yang, R.; Sun, X.; Xing, C.; Maturura, E. An ambient pressure method for synthesizing NaY zeolite. Microporous Mesoporous Mater. 2021, 320, 111073. [Google Scholar] [CrossRef]
  44. Ferraria, A.M.; Carapeto, A.P.; Botelho do Rego, A.M. X-ray photoelectron spectroscopy: Silver salts revisited. Vacuum 2012, 86, 1988–1991. [Google Scholar] [CrossRef]
  45. Jacobs, P.A.; Uytterhoeven, J.B.; Beyer, H.K. Some unusual properties of activated and reduced AgNaA zeolites. J. Chem. Soc. Faraday Trans. 1979, 75, 56–64. [Google Scholar] [CrossRef]
  46. Jacobs, P.A.; Uytterhoeven, J.B.; Beyer, H.K. Cleavage of Water Over Zeolites. J. Chem. Soc. Chem. Commun. 1977, 128–129. [Google Scholar] [CrossRef]
  47. Fang, H.; Wang, C.; Li, D.; Zhou, S.; Du, Y.; Zhang, H.; Hang, C.; Tian, Y.; Suga, T. Fabrication of Ag@Ag2O-MnOx composite nanowires for high-efficient room-temperature removal of formaldehyde. J. Mater. Sci. Technol. 2021, 91, 5–16. [Google Scholar] [CrossRef]
  48. Shin, S.; Song, J. Modeling and simulations of the removal of formaldehyde using silver nano-particles attached to granular activated carbon. J. Hazard. Mater. 2011, 194, 385–392. [Google Scholar] [CrossRef] [PubMed]
Figure 1. Raman spectra of LiY and NaY (a), XRD patterns (b), XPS survey spectra (c), and Na, Li, and Ag atomic contents (d) of NaY, LiY, NaYAg, and LiYAg, respectively.
Figure 1. Raman spectra of LiY and NaY (a), XRD patterns (b), XPS survey spectra (c), and Na, Li, and Ag atomic contents (d) of NaY, LiY, NaYAg, and LiYAg, respectively.
Nanomaterials 12 03215 g001
Figure 2. PLE (a) and PL (b) spectra of Ag CLs in LiYAg and NaYAg, respectively, under 306 nm excitation; inset: corresponding normalized PL spectra.
Figure 2. PLE (a) and PL (b) spectra of Ag CLs in LiYAg and NaYAg, respectively, under 306 nm excitation; inset: corresponding normalized PL spectra.
Nanomaterials 12 03215 g002
Figure 3. High-resolution XPS spectra of Ag 3d (a) and background-corrected Auger spectra of Ag MNN (b) in LiYAg and NaYAg, respectively.
Figure 3. High-resolution XPS spectra of Ag 3d (a) and background-corrected Auger spectra of Ag MNN (b) in LiYAg and NaYAg, respectively.
Nanomaterials 12 03215 g003
Figure 4. PL spectra of LiYAg (a) and NaYAg (b) before and after exposing to different contents of formaldehyde atmospheres; digital photographs of LiYAg and NaYAg after exposing to different contents of formaldehyde atmospheres under natural light (c); relative emission intensity of LiYAg and NaYAg at increasing contents of formaldehyde gases (d).
Figure 4. PL spectra of LiYAg (a) and NaYAg (b) before and after exposing to different contents of formaldehyde atmospheres; digital photographs of LiYAg and NaYAg after exposing to different contents of formaldehyde atmospheres under natural light (c); relative emission intensity of LiYAg and NaYAg at increasing contents of formaldehyde gases (d).
Nanomaterials 12 03215 g004
Figure 5. UV–vis absorbance spectra of LiYAg and NaYAg before and after exposing in different formaldehyde atmospheres.
Figure 5. UV–vis absorbance spectra of LiYAg and NaYAg before and after exposing in different formaldehyde atmospheres.
Nanomaterials 12 03215 g005
Figure 6. Auger parameter of Ag MNN in LiYAg and NaYAg before and after exposing in different formaldehyde-content atmospheres.
Figure 6. Auger parameter of Ag MNN in LiYAg and NaYAg before and after exposing in different formaldehyde-content atmospheres.
Nanomaterials 12 03215 g006
Publisher’s Note: MDPI stays neutral with regard to jurisdictional claims in published maps and institutional affiliations.

Share and Cite

MDPI and ACS Style

Yu, J.; Ye, S.; Xv, X.; Pan, L.; Lin, P.; Liao, H.; Wang, D. Thermal-Driven Formation of Silver Clusters Inside Na/Li FAUY Zeolites for Formaldehyde Detection. Nanomaterials 2022, 12, 3215. https://doi.org/10.3390/nano12183215

AMA Style

Yu J, Ye S, Xv X, Pan L, Lin P, Liao H, Wang D. Thermal-Driven Formation of Silver Clusters Inside Na/Li FAUY Zeolites for Formaldehyde Detection. Nanomaterials. 2022; 12(18):3215. https://doi.org/10.3390/nano12183215

Chicago/Turabian Style

Yu, Jianzhong, Song Ye, Xinling Xv, Ling Pan, Peixuan Lin, Huazhen Liao, and Deping Wang. 2022. "Thermal-Driven Formation of Silver Clusters Inside Na/Li FAUY Zeolites for Formaldehyde Detection" Nanomaterials 12, no. 18: 3215. https://doi.org/10.3390/nano12183215

Note that from the first issue of 2016, this journal uses article numbers instead of page numbers. See further details here.

Article Metrics

Back to TopTop