Next Article in Journal
Molecular Simulation of External Electric Fields on the Crystal State: A Perspective
Next Article in Special Issue
Statistical Theory of Helical Twisting in Nematic Liquid Crystals Doped with Chiral Nanoparticles
Previous Article in Journal
Influences of Sn on Properties of Ag-Based and Cu-Based Brazing Filler Metals
Previous Article in Special Issue
Backbone Conformation Shifts in X-ray Structures of Human Acetylcholinesterase upon Covalent Organophosphate Inhibition
 
 
Font Type:
Arial Georgia Verdana
Font Size:
Aa Aa Aa
Line Spacing:
Column Width:
Background:
Article

M-Center in Neutron-Irradiated 4H-SiC

1
Ruđer Bošković Institute, Bijenička cesta 54, 10000 Zagreb, Croatia
2
National Institutes for Quantum and Radiological Science and Technology, 1233 Watanuki, Takasaki 370-1292, Japan
3
Jožef Stefan Institute, Jamova cesta 39, 1000 Ljubljana, Slovenia
*
Author to whom correspondence should be addressed.
Crystals 2021, 11(11), 1404; https://doi.org/10.3390/cryst11111404
Submission received: 22 October 2021 / Revised: 14 November 2021 / Accepted: 17 November 2021 / Published: 18 November 2021

Abstract

:
We report on the metastable defects introduced in the n-type 4H-SiC material by epithermal and fast neutron irradiation. The epithermal and fast neutron irradiation defects in 4H-SiC are much less explored compared to electron or proton irradiation-induced defects. In addition to the carbon vacancy (Vc), silicon vacancy (Vsi) and carbon antisite-carbon vacancy (CAV) complex, the neutron irradiation has introduced four deep-level defects, all arising from the metastable defect, the M-center. The metastable deep-level defects were investigated by deep level transient spectroscopy (DLTS), high-resolution Laplace DLTS (L-DLTS) and isothermal DLTS. The existence of the fourth deep-level defect, M4, recently observed in ion-implanted 4H-SiC, has been additionally confirmed in neutron-irradiated samples. The isothermal DLTS technique has been proven as a useful tool for studying the metastable defects.

1. Introduction

The metastable defects whose configuration depends on bias and/or thermal treatments, and whose behavior was not always easily or fully understood, have a special place in studying the deep-level defects in semiconductors. One of those bi-stable defects is the M-center in 4H-SiC material, reported for the first time almost two decades ago [1]. Since then, M-center has been observed upon the low energy electron irradiation [2,3], 2.5 MeV proton irradiation [1,4,5,6] and 2 MeV He ion implantation [7] of n-type 4H-SiC. Comprehensive experimental studies and analyses have been performed using mostly the deep-level transient spectroscopy (DLTS).
The M-center in n-type 4H-SiC is a bi-stable defect whose configuration depends on bias and thermal treatments imposed on the samples. Therefore, by adjusting the bias and following well-defined annealing procedures [7], M-center can be placed in a selected configuration before DLTS measurement. It has been widely accepted among the research community to refer to the M-center configurations as A and B.
Since the first published reports of the M-center, three deep-level defects were assigned to it. The M1 (0.41–0.43 eV) and M3 (0.75–0.9 eV) deep levels were observed in configuration A, while the M2 (0.63–0.70 eV) deep level was observed in configuration B [1,2,3,4,5,6]. In addition to these three deep levels arising from the M-center, Nielsen et al. [6] have proposed the existence of a fourth deep level in configuration B and labeled it as M4. However, due to the technical limitations of DLTS, i.e., the fact that the technique itself involves a temperature scan, the M4 deep level was not accessible for many years.
Recently, Coutinho et al. [8] provided the direct evidence on the existence of the M4 (0.86 eV) deep level in 4H-SiC. Combining the advanced first-principles calculations and isothermal DLTS, it was demonstrated that the properties of M-center, including bistability, annealing, reconfiguration kinetics and electronic levels, match those of the carbon self-interstitial.
In this work, we have applied DLTS, high-resolution Laplace DLTS (L-DLTS) and isothermal DLTS to study the metastable defects in 4H-SiC material introduced by epithermal and fast neutron irradiation. The main aim of this work is to investigate the much less studied neutron irradiation induced defects primarily due to the growing interest and applications of 4H-SiC materials for neutron detection [9]. In addition, our intention is to compare these findings with the recently published study on ion implantation induced defects and to further explore the possibilities of isothermal DLTS technique.

2. Materials and Methods

For this study, we have used n-type nitrogen-doped 4H-SiC epitaxial layers, 25 µm thick. The epilayers were grown on an 8° off-cut silicon face of a 350 µm thick 4H-SiC (0001) wafer without a buffer layer. The Schottky barriers diodes (SBDs) were formed by thermal evaporation of nickel through a metal mask with a patterned square aperture of 1 mm × 1 mm, while Ohmic contacts were formed on the backside of the silicon carbide substrate by nickel sintering at 950 °C in an Ar atmosphere.
The SBDs were irradiated with epithermal and fast neutrons at the Jozef Stefan Institute (JSI) TRIGA reactor in Ljubljana, Slovenia. The selected neutron fluence was 1013 cm−2. Thermal neutrons with energy less than 0.55 eV were filtered by irradiating the Schottky barrier diodes inside a cadmium box with a wall thickness of 1 mm. The neutron energy spectrum and irradiation settings are the same as in the previously reported study [10]. Figure 1 displays the neutron spectra in the pneumatic tube (PT) irradiation channel, located in the F-24 core position, obtained by Monte Carlo simulation using the MCNP code and subsequently characterized based on experimental neutron activation measurements. More details are given elsewhere [10].
The temperature-dependent current-voltage (I-V-T) and capacitance-voltage (C-V-T) measurements were performed by a Keithley 4200 SCS (Keithley Instruments, Cleveland, OH, USA). DLTS, L-DLTS and isothermal DLTS measurements were performed using a Boonton 7200 capacitance meter (Boonton Electronics, New York, NY, USA) and NI PCI-6521 data acquisition device (NI, Austin, TX, USA). Reverse bias and electrical filling pulses were applied to the SBDs using the analog output of the acquisition device. The stable temperature control of the SBD in OptistatDN cryostat (Oxford Instruments, Oxfordshire, England) was realized using Lakeshore 332 and Lakeshore 335 temperature controllers (Lake Shore Cryotronics, Inc., Westerville, OH, USA). The sample temperature was constant during isothermal DLTS measurements, changing less than 0.05 K. The isothermal DLTS technique is a very useful technique which enables studies of the deep-level transformation kinetics at the same temperature [11].
Three different annealing procedures were used to control the configuration of the M-center prior to measurements. Detailed descriptions on annealing procedures are given elsewhere [7].

3. Results and Discussion

Figure 2 shows the free-carrier concentration profiles of as-grown, 2 MeV He ion-implanted and epithermal and fast neutron-irradiated n-type 4H-SiC samples (solid lines, left y axis) and the calculated vacancy concentration profiles (dashed lines, right y axis). More details on 2 MeV He ion implantation are given in a previous study [7].
The displacement damage profiles, i.e., the vacancy concentration profiles, are simulated using the SRIM code [12] and FLUKA software [13] for the ion-implanted and neutron-irradiated 4H-SiC, respectively. The averaged primary displacement (vacancy) generation rate (VGR) distribution, created in collision cascades of the 2.0 MeV He ions being implanted in the 4H-SiC epitaxial layer at normal incident not aligned with the crystal axis, was simulated for a total of 10,000 ions using the SRIM code. The displacement damage introduced by neutron irradiation in the 4H-SiC epitaxial layer was simulated by Fluka software. The neutron spectrum shown in Figure 1 (blue line) was used to select the neutron energies used in the simulation (627 values in the range 2 × 10−4–2 × 107 eV) and to calculate the average displacement generation rate. A total of 106 incident neutrons were simulated for each energy. More details on simulations using SRIM code and FLUKA software are given elsewhere [10].
As expected, the free carrier concentration profiles are significantly different in ion-implanted and neutron-irradiated samples. The reason is that epithermal and fast neutron irradiation introduces damage homogenously through the volume, while the ion implantation introduces damage with a well-defined depth profile (Figure 2). To avoid the 2 MeV He ion projected range at 4.8 µm, a reverse voltage of −4 V corresponding to a depletion width of <4 µm was selected for DLTS measurements [7]. Such restrictions are redundant in the case of neutron-irradiated samples, where a reverse voltage up to −10 V was used.
The reasons why we have selected epithermal and fast neutrons to introduce deep-level defects in 4H-SiC material are multiple, the growing interest in neutron radiation detection based on 4H-SiC material being just one of them [9]. Additional reasons are (i) the homogenously distributed damage through the volume (as clearly shown in Figure 2), which is rather important for techniques such as DLTS (that scans over volume), and (ii) the fact that epithermal and fast neutron irradiation introduces the same electrically active defects as ion implantation into 4H-SiC [10]. Those defects are known as S1 (0.40 eV) and S2 (0.70 eV), and are already assigned to VSi (−3/=) and VSi (=/−) charge state transitions of the silicon vacancy [14], respectively.
Figure 3 shows DLTS spectra for the neutron-irradiated sample in two configurations, A and B. The M-center was transformed to configuration B or configuration A by annealing at 450 K (for 20 min) and cooling down without applying bias (0 V) or by 20 min annealing at the temperature of 340 K and cooling down with the applied bias (−30 V), respectively.
In addition to a well-known Z1/2 deep-level defect assigned to a transition between double negative and neutral charge state of carbon vacancy VC (=/0) [15], three deep levels with activation energies of 0.4, 0.7 and 0.9 eV below the conduction band minimum are detected. Two deep levels at 0.4 and 0.7 eV are assigned to the already-mentioned S1 and S2, while the 0.9 eV deep level, labeled as EH4, is assigned to different configurations of the (−/0) charge transition of the carbon antisite-carbon vacancy (CAV) complex [16].
The M1 and M3 deep levels observed in configuration A overlap with S1 and S2 deep levels, while the M2 deep level observed in configuration B overlaps with Z1/2. This result is consistent with previously published DLTS results on 2 MeV He ion implantation-induced defects [7].
To obtain more information about the metastable defects in neutron-irradiated samples, we have applied L-DLTS to investigate S1 and M1 deep-level defects. Figure 4 shows L-DLTS spectra for neutron-irradiated sample measured in configurations A and B. While keeping the sample in configuration B (only S1 deep level is detected), two emission lines arising from S1 are observed. The S1 Laplace emission line splitting has already been reported [14]. The situation has slightly changed as we have set the sample in configuration A. As expected, (see Figure 3), the signal due to the M1 deep level is rising, and it overlaps with one of the S1 Laplace emission lines (Figure 4). To the best of our knowledge, this is the first time a metastable defect in 4H-SiC has been observed by L-DLTS.
According to the modeling studies [8], the M1 deep level is assigned to the carbon self-interstitial (Ci) residing on the hexagonal lattice site (-h). If the S1 emission lines splitting (S11 and S12 in Figure 4) corresponds to silicon vacancies (VSi) residing on two different lattice sites, such as the carbon vacancy (Vc) [17], then we can assign two observed L-DLTS emission lines S11 and S12 to VSi residing on two lattices sites, cubic (-k) and hexagonal (-h), respectively, while the M1 deep level resides on the hexagonal (-h) lattice site.
To compare the M1 deep level in the 2 MeV He ion implanted with epithermal and fast neutron-irradiated 4H-SiC in more detail, the isothermal DLTS has been applied. Figure 5 shows isothermal DLTS signals measured in configurations A and B. M-center was first placed in configuration B by annealing without bias at 450 K for 20 min, which was followed by cooling down without bias and a 20 min long waiting period at a measurement temperature. Next, M-center was placed in configuration A by applying reverse bias (−30 V) at a temperature of 340 K (for 20 min) and cooling down under reverse bias (−30 V) to the measurement temperature. The overlap of S1 and M1 is observed in configuration A, while the signal in configuration B is only due to the S1 deep level.
To get a “clean” signal coming only from the metastable defects, we have used the difference isothermal DLTS signal. The difference isothermal DLTS signal is obtained by subtracting isothermal DLTS spectra measured with M-center in configuration A and configuration B (Figure 5). Such representation enables more accurate analysis, needed for deep-level defect parameter estimations, such as activation energy, capture cross section and concentration. More details on the analysis of isothermal DLTS data are given elsewhere [7]. Here, we provide an additional way of presenting isothermal DLTS signal using 2D plots.
Figure 6 shows heatmap plots of the difference in isothermal DLTS signal for (a) neutron-irradiated (Figure 5) and (b) ion-implanted samples (not shown here, see Ref. [7] for more details). As seen in Figure 6, the M1 signal is almost identical in both cases.
The M1 deep level was studied by L-DLTS and isothermal DLTS, and the results clearly showed that M1 is indeed the same defect in both neutron-irradiated and ion-implanted samples; thus, we can move to a more complex situation, where the rest of M deep-level defects (M2, M3 and M4) overlap with Z1/2, S2 and EH4. Unfortunately, due to the several closely spaced deep levels, L-DLTS cannot provide additional and accurate information. Therefore, we will focus on isothermal DLTS.
Figure 7a shows isothermal DLTS spectra of neutron-irradiated sample with the M-center placed in configuration A and configuration B. The M2 and M4 deep levels observed in configuration B overlap with Z1/2 and EH4 deep levels, while the M3 deep level observed in configuration A overlaps with S2 deep level. From the difference isothermal DLTS signal (Figure 7b), we can clearly detect signals due to the M2, M3 and M4 deep levels.
As seen in Figure 7b, the existence of the M4 deep level is once again confirmed using the isothermal DLTS. The obtained spectra match previously reported spectra in case of 2 MeV He ion implantation [7]. Using all the above mention techniques, we have estimated activation energies for metastable defects as follows: M1 (0.41–0.43 eV), M2 (0.64–0.70 eV) and M3 (~0.72 eV). The activation energy for M4 could not be accurately estimated due to the signal broadening. There are two possible explanations for this, i.e., (i) the emission rate for M4 is too close to the reconfiguration rate from configuration B to configuration A and (ii) neutron irradiation has introduced more damage into the material (compared to 2 MeV He ion implantation), which has introduced more stress into the material and increased the broadening of DLTS and isothermal DLTS signals [18].
The presented results, using the neutron irradiation, are consistent with all previously obtained and reported results on metastable defects in 4H-SiC using the low electron energy irradiation, proton irradiation and ion implantation [1,2,3,4,5,6,7]. Moreover, these results are consistent with the first-principal calculations of M-center [8]. The presented data reconfirm the previously made assignment of the M center to the carbon interstitial.

4. Conclusions

We have investigated the M-center introduced in 4H-SiC by epithermal and fast neutron irradiation. Deep-level defects arising from the metastable M-center were studied by means of junction transient techniques, DLTS, L-DLTS and isothermal DLTS. We have confirmed the existence of the fourth deep-level defect, M4, already detected in ion-implanted 4H-SiC samples. Moreover, we have provided additional example of functionality of isothermal DLTS technique in studying the metastable deep-level defects.

Author Contributions

Formal analysis, T.B.; investigation, T.B., I.C., T.M., V.R. and L.S.; resources, T.M., V.R. and L.S.; writing—original draft preparation, I.C.; writing—review and editing, T.B., I.C., V.R., L.S. and T.M. All authors have read and agreed to the published version of the manuscript.

Funding

The present work was financially supported by the NATO Science for Peace and Security Programme, project no. G5674. The RBI project team would like to acknowledge financial support from the European Regional Development Fund for the Center of Excellence for Advanced Materials and Sensing Devices (Grant No. KK.01.1.1.01.0001).

Institutional Review Board Statement

Not applicable.

Informed Consent Statement

Not applicable.

Data Availability Statement

Data are contained within the article.

Acknowledgments

We would like to acknowledge Hidekazu Tsuchida and Norihiro Hoshino Central Research Institute of Electric Power Industry for the supply of SiC substrates with epitaxially grown 4H–SiC single-crystal layers.

Conflicts of Interest

The authors declare no conflict of interest.

References

  1. Nielsen, H.K.; Martin, D.M.; Lévêque, P.; Hallén, A.; Svensson, B.G. Annealing study of a bistable defect in proton-implanted n-type 4H-SiC. Phys. B Condens. Matter 2003, 340, 743–747. [Google Scholar] [CrossRef]
  2. Beyer, F.C.; Hemmingsson, C.G.; Pedersen, H.; Henry, A.; Isoya, J.; Morishita, N.; Ohshima, T.; Janzén, E. Bistable defects in low-energy electron irradiated n-type 4H-SiC. Phys. Status Solidi Rapid Res. Lett. 2010, 4, 227–229. [Google Scholar] [CrossRef]
  3. Beyer, F.C.; Hemmingsson, C.; Pedersen, H.; Henry, A.; Janzén, E.; Isoya, J.; Morishita, N.; Ohshima, T. Annealing behavior of the EB-centers and M-center in low-energy electron irradiated n -type 4H-SiC. J. Appl. Phys. 2011, 109, 103703. [Google Scholar] [CrossRef] [Green Version]
  4. Martin, D.M.; Kortegaard Nielsen, H.; Lévêque, P.; Hallén, A.; Alfieri, G.; Svensson, B.G. Bistable defect in mega-electron-volt proton implanted 4H silicon carbide. Appl. Phys. Lett. 2004, 84, 1704–1706. [Google Scholar] [CrossRef]
  5. Nielsen, H.K.; Hallén, A.; Martin, D.M.; Svensson, B.G. M-center in low-dose proton implanted 4H-SiC; Bistability and change in emission rate. Mater. Sci. Forum 2005, 483, 497–500. [Google Scholar] [CrossRef]
  6. Nielsen, H.K.; Hallén, A.; Svensson, B.G. Capacitance transient study of the metastable M center in n -type 4H-SiC. Phys. Rev. B Condens. Matter Mater. Phys. 2005, 72, 085208. [Google Scholar] [CrossRef]
  7. Capan, I.; Brodar, T.; Bernat, R.; Pastuović, Ž.; Makino, T.; Ohshima, T.; Gouveia, J.D.; Coutinho, J. M-center in 4H-SiC: Isothermal DLTS and first principles modeling studies. J. Appl. Phys. 2021, 130, 125703. [Google Scholar] [CrossRef]
  8. Coutinho, J.; Gouveia, J.D.; Makino, T.; Ohshima, T.; Pastuović, Ž.; Bakrač, L.; Brodar, T.; Capan, I. M center in 4H-SiC is a carbon self-interstitial. Phys. Rev. B 2021, 103, L180102. [Google Scholar] [CrossRef]
  9. Coutinho, J.; Torres, V.J.B.; Capan, I.; Brodar, T.; Ereš, Z.; Bernat, R.; Radulović, V. Silicon carbide diodes for neutron detection. Nucl. Inst. Methods Phys. Res. A 2020, 986, 164793. [Google Scholar] [CrossRef]
  10. Brodar, T.; Bakrač, L.; Capan, I.; Ohshima, T.; Snoj, L.; Radulović, V.; Pastuović, Ž. Depth Profile Analysis of Deep Level Defects in 4H-SiC Introduced by Radiation. Crystals 2020, 10, 845. [Google Scholar] [CrossRef]
  11. Tokuda, Y. Transformation behavior of room-temperature-stable metastable defects in hydrogen-implanted n-type silicon studied by isothermal deep-level transient spectroscopy. J. Appl. Phys. 2006, 100, 023704. [Google Scholar] [CrossRef]
  12. Ziegler, J.F.; Ziegler, M.D.; Biersack, J.P. SRIM—The stopping and range of ions in matter (2010). Nucl. Instrum. Methods Phys. Res. Sect. B Beam Interact. Mater. Atoms 2010, 268, 1818–1823. [Google Scholar] [CrossRef] [Green Version]
  13. Battistoni, G.; Cerutti, F.; Fassò, A.; Ferrari, A.; Muraro, S.; Ranft, J.; Roesler, S.; Sala, P.R. The FLUKA code: Description and benchmarking. AIP Conf. Proc. 2007, 896, 31–49. [Google Scholar]
  14. Bathen, M.E.; Galeckas, A.; Müting, J.; Ayedh, H.M.; Grossner, U.; Coutinho, J.; Frodason, Y.K.; Vines, L. Electrical charge state identification and control for the silicon vacancy in 4H-SiC. NPJ Quantum Inf. 2019, 5, 111. [Google Scholar] [CrossRef] [Green Version]
  15. Son, N.T.; Trinh, X.T.; Løvlie, L.S.; Svensson, B.G.; Kawahara, K.; Suda, J.; Kimoto, T.; Umeda, T.; Isoya, J.; Makino, T.; et al. Negative-U System of Carbon Vacancy in 4H-SiC. Phys. Rev. Lett. 2012, 109, 187603. [Google Scholar] [CrossRef] [PubMed] [Green Version]
  16. Karsthof, R.; Bathen, M.E.; Galeckas, A.; Vines, L. Conversion pathways of primary defects by annealing in proton-irradiated n-type 4H-SiC. Phys. Rev. B 2020, 102, 184111. [Google Scholar] [CrossRef]
  17. Capan, I.; Brodar, T.; Coutinho, J.; Ohshima, T.; Markevich, V.P.; Peaker, A.R. Acceptor levels of the carbon vacancy in 4 H -SiC: Combining Laplace deep level transient spectroscopy with density functional modeling. J. Appl. Phys. 2018, 124, 245701. [Google Scholar] [CrossRef] [Green Version]
  18. Brodar, T.; Capan, I.; Radulović, V.; Snoj, L.; Pastuović, Z.; Coutinho, J.; Ohshima, T. Laplace DLTS study of deep defects created in neutron-irradiated n-type 4H-SiC. Nucl. Instrum. Methods Phys. Res. Sect. B Beam Interact. Mater. Atoms 2018, 437, 27–31. [Google Scholar] [CrossRef] [Green Version]
Figure 1. Neutron spectra in the Jozef Stefan Institute (JSI) TRIGA pneumatic tube (PT) irradiation channel, corresponding to bare and Cd-covered irradiations, obtained by means of Monte Carlo simulations and subsequently characterized based on experimental neutron activation measurements.
Figure 1. Neutron spectra in the Jozef Stefan Institute (JSI) TRIGA pneumatic tube (PT) irradiation channel, corresponding to bare and Cd-covered irradiations, obtained by means of Monte Carlo simulations and subsequently characterized based on experimental neutron activation measurements.
Crystals 11 01404 g001
Figure 2. Free-carrier concentration profiles of as-grown, ion-implanted and neutron-irradiated n-type 4H-SiC samples (solid lines, left y axis). The calculated vacancy concentration profiles estimated for 2 MeV He ions using SRIM code (blue, dashed, right y axis) and for neutrons using FLUKA (red, dashed, right y axis). The free carrier concentration profiles are obtained from the C–V measurements.
Figure 2. Free-carrier concentration profiles of as-grown, ion-implanted and neutron-irradiated n-type 4H-SiC samples (solid lines, left y axis). The calculated vacancy concentration profiles estimated for 2 MeV He ions using SRIM code (blue, dashed, right y axis) and for neutrons using FLUKA (red, dashed, right y axis). The free carrier concentration profiles are obtained from the C–V measurements.
Crystals 11 01404 g002
Figure 3. DLTS spectra of neutron-irradiated 4H-SiC samples in two configurations of the M-center, configuration A (red, solid) and configuration B (blue, dashed).
Figure 3. DLTS spectra of neutron-irradiated 4H-SiC samples in two configurations of the M-center, configuration A (red, solid) and configuration B (blue, dashed).
Crystals 11 01404 g003
Figure 4. Laplace DLTS spectra for neutron-irradiated samples in configurations A (red, solid) and B (blue, dashed), measured at 210 K.
Figure 4. Laplace DLTS spectra for neutron-irradiated samples in configurations A (red, solid) and B (blue, dashed), measured at 210 K.
Crystals 11 01404 g004
Figure 5. Isothermal DLTS spectra for neutron-irradiated 4H-SiC samples with M-center in configurations A (red, solid) and B (blue, dashed). Measurements are done at 180 K.
Figure 5. Isothermal DLTS spectra for neutron-irradiated 4H-SiC samples with M-center in configurations A (red, solid) and B (blue, dashed). Measurements are done at 180 K.
Crystals 11 01404 g005
Figure 6. Heatmap plots of differential isothermal DLTS signals for (a) neutron-irradiated and (b) ion-implanted 4H-SiC samples.
Figure 6. Heatmap plots of differential isothermal DLTS signals for (a) neutron-irradiated and (b) ion-implanted 4H-SiC samples.
Crystals 11 01404 g006
Figure 7. (a) Isothermal DLTS spectra for neutron-irradiated 4H-SiC sample with M-center in configurations A (red, solid) and B (blue, dashed) measured at 300 K. (b) Different isothermal DLTS signals (configuration A-configuration B).
Figure 7. (a) Isothermal DLTS spectra for neutron-irradiated 4H-SiC sample with M-center in configurations A (red, solid) and B (blue, dashed) measured at 300 K. (b) Different isothermal DLTS signals (configuration A-configuration B).
Crystals 11 01404 g007
Publisher’s Note: MDPI stays neutral with regard to jurisdictional claims in published maps and institutional affiliations.

Share and Cite

MDPI and ACS Style

Capan, I.; Brodar, T.; Makino, T.; Radulovic, V.; Snoj, L. M-Center in Neutron-Irradiated 4H-SiC. Crystals 2021, 11, 1404. https://doi.org/10.3390/cryst11111404

AMA Style

Capan I, Brodar T, Makino T, Radulovic V, Snoj L. M-Center in Neutron-Irradiated 4H-SiC. Crystals. 2021; 11(11):1404. https://doi.org/10.3390/cryst11111404

Chicago/Turabian Style

Capan, Ivana, Tomislav Brodar, Takahiro Makino, Vladimir Radulovic, and Luka Snoj. 2021. "M-Center in Neutron-Irradiated 4H-SiC" Crystals 11, no. 11: 1404. https://doi.org/10.3390/cryst11111404

Note that from the first issue of 2016, this journal uses article numbers instead of page numbers. See further details here.

Article Metrics

Back to TopTop